daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Polarons, Bipolarons, And Absorption Spectroscopy of PEDOT AITranslate

Linköping University; Linköping University; Linköping University; Linköping University; Linköping University; Linköping University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Electronic structure and optical absorption spectra of poly(3,4-ethylenedioxythiophene) (PEDOT) for different oxidation levels were studied using density functional theory (DFT) and time-dependent DFT. It is shown, that the DFT-based predictions for the polaronic and bipolaronic states and the nature of corresponding optical transitions are qualitatively different from the widely used traditional picture based on semi-empirical pre-DFT approaches that still dominate the current literature. On the basis of the results of our calculations, the experimental Vis/NIR absorbance spectroscopy and the electron paramagnetic resonance spectroscopy are re-examined, and a new interpretation of the measured spectra and the spin signal, which is qualitatively different from the traditional interpretation, is provided. The findings and conclusions concerning the nature of polaronic and bipolaronic states, band structure and absorption spectra presented for PEDOT, are generic for a wide class of conducting polymers (such as polythiophenes and their derivatives) that have a similar structure of monomer units.

KeyWords AITranslate

polarons bipolarons conducting polymers PEDOT Vis/NIR absorbance spectroscopy electron paramagnetic resonance Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.8b00061

Chinese Library Classification Number:

Citation Information:

Electronic structure and optical absorption spectra of poly(3,4-ethylenedioxythiophene) (PEDOT) for different oxidation levels were studied using density functional theory (DFT) and time-dependent DFT. It is shown, that the DFT-based predictions for the polaronic and bipolaronic states and the nature of corresponding optical transitions are qualitatively different from the widely used traditional picture based on semi-empirical pre-DFT approaches that still dominate the current literature. On the basis of the results of our calculations, the experimental Vis/NIR absorbance spectroscopy and the electron paramagnetic resonance spectroscopy are re-examined, and a new interpretation of the measured spectra and the spin signal, which is qualitatively different from the traditional interpretation, is provided. The findings and conclusions concerning the nature of polaronic and bipolaronic states, band structure and absorption spectra presented for PEDOT, are generic for a wide class of conducting polymers (such as polythiophenes and their derivatives) that have a similar structure of monomer units.

quote

GB/T 7714-2015 [1] Igor Zozoulenko, Amritpal Singh, Sandeep Kumar Singh, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00061.
MLA [1] Igor Zozoulenko, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00061.
APA [1] Igor Zozoulenko, Amritpal Singh, Sandeep Kumar Singh, Viktor Gueskine, Xavier Crispin, & Magnus Berggren. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00061
IEEE [1] Igor Zozoulenko, Amritpal Singh, Sandeep Kumar Singh, Viktor Gueskine, Xavier Crispin, and Magnus Berggren, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00061. keywords: {polarons;bipolarons;conducting polymers;PEDOT;Vis/NIR absorbance spectroscopy;electron paramagnetic resonance;Show More}