Spotlighting graphene quantum dots and beyond: Synthesis, properties and sensing applications AITranslate

CSIR-Central Electrochemical Research Institute;CSIR-Central Electrochemical Research Institute;CSIR-Central Electrochemical Research Institute
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Graphene quantum dot (GQDs) is a zero dimensional member in the carbon family and is usually considered as a chopped fragment from a graphene sheet. The unique features exhibited by GQDs are due to the combined structural properties of graphene endowed with the edge effects and quantum confinement properties. As a result, GQDs find widespread applications in biosensing, bioimaging, drug delivery, solar cells, photo detectors, batteries, light emitting diodes, supercapacitors etc. In this review, our first key focus is on various top-down and bottom-up approach employed for the synthesis of engineered GQDs. Following this, a brief discussion on the post treatment methods available for the purification of the GQDs is also presented. Sensors based on quantum dots systems of transition metal dichalcogenides (TMDs) are also briefly discussed. The key focus in this review is on the usefulness of the engineered/hetero atom-doped GQDs and TMDQDs in optical and electrochemical sensor design and their applications during chemical and bioanalysis. Finally, we have also briefly mentioned about the existing bottlenecks in the sensors fabrication and a perspective to overcome the odds.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2017.09.002

Chinese Library Classification Number:

Citation Information:

Graphene quantum dot (GQDs) is a zero dimensional member in the carbon family and is usually considered as a chopped fragment from a graphene sheet. The unique features exhibited by GQDs are due to the combined structural properties of graphene endowed with the edge effects and quantum confinement properties. As a result, GQDs find widespread applications in biosensing, bioimaging, drug delivery, solar cells, photo detectors, batteries, light emitting diodes, supercapacitors etc. In this review, our first key focus is on various top-down and bottom-up approach employed for the synthesis of engineered GQDs. Following this, a brief discussion on the post treatment methods available for the purification of the GQDs is also presented. Sensors based on quantum dots systems of transition metal dichalcogenides (TMDs) are also briefly discussed. The key focus in this review is on the usefulness of the engineered/hetero atom-doped GQDs and TMDQDs in optical and electrochemical sensor design and their applications during chemical and bioanalysis. Finally, we have also briefly mentioned about the existing bottlenecks in the sensors fabrication and a perspective to overcome the odds.

quote

GB/T 7714-2015 [1] Manila Ozhukil Valappil, Vijayamohanan K. Pillai, Subbiah Alwarappan. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.09.002.
MLA [1] Manila Ozhukil Valappil, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.09.002.
APA [1] Manila Ozhukil Valappil, Vijayamohanan K. Pillai, & Subbiah Alwarappan. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.09.002
IEEE [1] Manila Ozhukil Valappil, Vijayamohanan K. Pillai, and Subbiah Alwarappan, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.09.002.