daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Polyhedral Oligomeric Silsesquioxanes (POSS)-Based Hybrid Soft Gels: Molecular Design, Material Advantages, and Emerging Applications AITranslate

National University of Singapore;Institute of High Performance Computing (IHPC); Zhejiang University School of Medicine;Institute of Materials Research and Engineering; National University of Singapore
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polyhedral oligomeric silsesquioxanes (POSS) represent the new frontier in hybrid materials science and engineering, because of their well-defined nanostructure and unique dual nature combining material properties from both inorganic siloxane cage and organic groups at the periphery. Recent advances in synthetic chemistry, combined with the controlled radical polymerization techniques, have significantly influenced the construction of POSS soft gel as emerging biomaterials and beyond. In this Review, the most recent developments in the design strategies of POSS-based hybrid soft gels are presented, with respect to different functions of architectural POSS, including POSS as a crosslinker, end-cap polymer chain, pendent group, etc. In addition, the insights into the uniqueness of POSS in microstructure and their different organic substituents in the enhancement of the hydrogel performance are illustrated. These sophisticated materials with multiple functions, oriented toward advanced therapeutic applications, are further summarized into several active domains in controlled drug delivery, 3D cell culture, tissue engineering, and wound healing. The recent new applications of using POSS hybrid soft gel in environmental health are also summarized in this Review. Finally, perspectives and challenges related to the further advancement of POSS-based hybrid soft gel materials are discussed.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.9b00491

Chinese Library Classification Number:

Citation Information:

Polyhedral oligomeric silsesquioxanes (POSS) represent the new frontier in hybrid materials science and engineering, because of their well-defined nanostructure and unique dual nature combining material properties from both inorganic siloxane cage and organic groups at the periphery. Recent advances in synthetic chemistry, combined with the controlled radical polymerization techniques, have significantly influenced the construction of POSS soft gel as emerging biomaterials and beyond. In this Review, the most recent developments in the design strategies of POSS-based hybrid soft gels are presented, with respect to different functions of architectural POSS, including POSS as a crosslinker, end-cap polymer chain, pendent group, etc. In addition, the insights into the uniqueness of POSS in microstructure and their different organic substituents in the enhancement of the hydrogel performance are illustrated. These sophisticated materials with multiple functions, oriented toward advanced therapeutic applications, are further summarized into several active domains in controlled drug delivery, 3D cell culture, tissue engineering, and wound healing. The recent new applications of using POSS hybrid soft gel in environmental health are also summarized in this Review. Finally, perspectives and challenges related to the further advancement of POSS-based hybrid soft gel materials are discussed.

quote

GB/T 7714-2015 [1] Huihui Shi, Jing Yang, Mingliang You, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.9b00491.
MLA [1] Huihui Shi, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.9b00491.
APA [1] Huihui Shi, Jing Yang, Mingliang You, Zibiao Li, & Chaobin He. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.9b00491
IEEE [1] Huihui Shi, Jing Yang, Mingliang You, Zibiao Li, and Chaobin He, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.9b00491.