Hollow Spherical Covalent Organic Frameworks from Nonplanar or Planar Monomers for the Fluorescence Detection of Telomere DNA: Role of the 2-(2-Azidoethoxy)ethoxy Group AITranslate

National Sun Yat-sen University;Inorganic Chemistry I, Technische Universität Dresden; National Sun Yat-sen University;Inorganic Chemistry I, Technische Universität Dresden; Assiut University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Construction of covalent organic frameworks (COFs) with a hollow and uniform morphology─regardless of whether planar or nonplanar building blocks are employed─is still challenging. Herein, we report a facile strategy for the self-assembly and template-free synthesis of hollow spherical COFs by increasing the percentage content of 2-(2-azidoethoxy)ethoxy groups in the pore skeleton of a COF. Moreover, the morphological diversity dependent on the percentage content of 2-(2-azidoethoxy)ethoxy groups in the COF structure is observed. COF-100%N3, which is formed by the polycondensation of the nonplanar 1,3,5-tris(4-aminophenyl)benzene monomer, having the highest percentage content of the 2-(2-azidoethoxy)ethoxy group (100%), is self-assembled into homogeneous hollow spheres. For the first time, our strategy effectively explores the self-assembly of the planar monomer into a hollow spherical COF. Hollow spherical TPP-COF-100%N3 is formed via the polycondensation of the planar 2,4,6-tris(4-aminophenyl)pyridine monomer and 2-(2-azidoethoxy)ethoxy group (100%). Due to the favorable characteristics of its specific surface area and hollow mesoporous nature, spherical COF-100%N3 functions as an enticing sensing platform for the fluorescence-selective and -sensitive detection of telomere DNA. Consequently, this research study documents a facile strategy for constructing a unique hollow spherical COF and expands the application of COFs as fluorescent platforms for DNA detection.

KeyWords AITranslate

covalent organic framework selfassembly hollow sphere fluorescence telomere DNA
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01460

Chinese Library Classification Number:

Citation Information:

Construction of covalent organic frameworks (COFs) with a hollow and uniform morphology─regardless of whether planar or nonplanar building blocks are employed─is still challenging. Herein, we report a facile strategy for the self-assembly and template-free synthesis of hollow spherical COFs by increasing the percentage content of 2-(2-azidoethoxy)ethoxy groups in the pore skeleton of a COF. Moreover, the morphological diversity dependent on the percentage content of 2-(2-azidoethoxy)ethoxy groups in the COF structure is observed. COF-100%N3, which is formed by the polycondensation of the nonplanar 1,3,5-tris(4-aminophenyl)benzene monomer, having the highest percentage content of the 2-(2-azidoethoxy)ethoxy group (100%), is self-assembled into homogeneous hollow spheres. For the first time, our strategy effectively explores the self-assembly of the planar monomer into a hollow spherical COF. Hollow spherical TPP-COF-100%N3 is formed via the polycondensation of the planar 2,4,6-tris(4-aminophenyl)pyridine monomer and 2-(2-azidoethoxy)ethoxy group (100%). Due to the favorable characteristics of its specific surface area and hollow mesoporous nature, spherical COF-100%N3 functions as an enticing sensing platform for the fluorescence-selective and -sensitive detection of telomere DNA. Consequently, this research study documents a facile strategy for constructing a unique hollow spherical COF and expands the application of COFs as fluorescent platforms for DNA detection.

quote

GB/T 7714-2015 [1] Lamiaa Reda Ahmed, Leisan Gilmanova, ChengTang Pan, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01460.
MLA [1] Lamiaa Reda Ahmed, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01460.
APA [1] Lamiaa Reda Ahmed, Leisan Gilmanova, ChengTang Pan, Stefan Kaskel, & Ahmed F. M. ELMahdy. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01460
IEEE [1] Lamiaa Reda Ahmed, Leisan Gilmanova, ChengTang Pan, Stefan Kaskel, and Ahmed F. M. ELMahdy, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01460. keywords: {covalent organic framework;selfassembly;hollow sphere;fluorescence;telomere DNA}