Polyselenonium Salt as a Heterogeneous Catalyst for Living/Controlled Cationic Polymerization AITranslate

Soochow University; Soochow University; Soochow University; Soochow University; Soochow University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Polyselenonium salt was synthesized by using functional polycaprolactone as a precursor for heterogeneous catalysis of living/controlled cationic polymerization of various vinyl ethers. Benefiting from the combination of the bench-stable polyselenonium salt and cationic RAFT agents, controlled cationic polymerization could be achieved under mild conditions such as room temperature, non-inert atmosphere, and the absence of rigorously monomer purification, yielding well-defined poly(vinyl ether)s with controlled molecular weights and low dispersity (Đ < 1.20). The heterogeneous catalyst can be easily separated by simple centrifugation and maintains catalytic efficiency above 90% even after six cycles of use, showing excellent reusability in subsequent polymerizations.

KeyWords AITranslate

living cationic polymerization selenonium salt heterogeneous catalysis cationic RAFT mild conditions
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01882

Chinese Library Classification Number:

Citation Information:

Polyselenonium salt was synthesized by using functional polycaprolactone as a precursor for heterogeneous catalysis of living/controlled cationic polymerization of various vinyl ethers. Benefiting from the combination of the bench-stable polyselenonium salt and cationic RAFT agents, controlled cationic polymerization could be achieved under mild conditions such as room temperature, non-inert atmosphere, and the absence of rigorously monomer purification, yielding well-defined poly(vinyl ether)s with controlled molecular weights and low dispersity (Đ < 1.20). The heterogeneous catalyst can be easily separated by simple centrifugation and maintains catalytic efficiency above 90% even after six cycles of use, showing excellent reusability in subsequent polymerizations.

quote

GB/T 7714-2015 [1] Xia Lin, Jiajia Li, Wenjing Shu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01882.
MLA [1] Xia Lin, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01882.
APA [1] Xia Lin, Jiajia Li, Wenjing Shu, Xiangqiang Pan, & Jian Zhu. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01882