Furanic (Meth)acrylate Monomers as Sustainable Reactive Diluents for Stereolithography AITranslate

North Dakota State University; North Dakota State University; North Dakota State University; North Dakota State University; North Dakota State University; North Dakota State University;Combat Capabilities Development Command Army Research Laboratory; North Dakota State University; North Dakota State University; North Dakota State University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We have successfully demonstrated the capability of six bioderived furanic (meth)acrylates to perform as reactive diluents in stereolithography resin compositions. Produced from 5-hydroxymethylfurfural, a biobased platform chemical, via a series of simple transformations, the furanic diluents can reduce the viscosity of commercial stereolithography resins, participate in photocuring with high conversion of polymerizable groups, and satisfy performance requirements. Compared to 1,6-hexanediol diacrylate, a widely used petroleum-based difunctional diluent, several furanic acrylate and methacrylate monomers offer significantly improved thermal and mechanical properties (glass transition temperature, Young’s modulus, tensile strength, tensile, and fracture toughness). Incorporating a long n-butyl substituent as a side chain into the diluent structure increases the fracture strain of the 3D printed samples compared to the unsubstituted counterpart but causes a reduction in strength, glass transition temperature, and thermal stability. Using an allyl group as a side chain improves the cross-link density of the system but increases brittleness. Of the six furanic diluents, 2,5-bis(hydroxymethyl)tetrahydrofuran diacrylate and 2,5-bis(hydroxymethyl)furan dimethacrylate demonstrated the best combination of properties. After the necessary optimization, the production of furanic (meth)acrylates has the potential to become more sustainable than the manufacturing of 1,6-hexanediol diacrylate. The potential for sustainability and the high performance of the biobased furanic monomers make them promising alternatives to petroleum-derived components in sustainable stereolithography resin compositions.

KeyWords AITranslate

acrylate methacrylate biobased monomer reactive diluent stereolithography 3D printing additive manufacturing BHMF
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02207

Chinese Library Classification Number:

Citation Information:

We have successfully demonstrated the capability of six bioderived furanic (meth)acrylates to perform as reactive diluents in stereolithography resin compositions. Produced from 5-hydroxymethylfurfural, a biobased platform chemical, via a series of simple transformations, the furanic diluents can reduce the viscosity of commercial stereolithography resins, participate in photocuring with high conversion of polymerizable groups, and satisfy performance requirements. Compared to 1,6-hexanediol diacrylate, a widely used petroleum-based difunctional diluent, several furanic acrylate and methacrylate monomers offer significantly improved thermal and mechanical properties (glass transition temperature, Young’s modulus, tensile strength, tensile, and fracture toughness). Incorporating a long n-butyl substituent as a side chain into the diluent structure increases the fracture strain of the 3D printed samples compared to the unsubstituted counterpart but causes a reduction in strength, glass transition temperature, and thermal stability. Using an allyl group as a side chain improves the cross-link density of the system but increases brittleness. Of the six furanic diluents, 2,5-bis(hydroxymethyl)tetrahydrofuran diacrylate and 2,5-bis(hydroxymethyl)furan dimethacrylate demonstrated the best combination of properties. After the necessary optimization, the production of furanic (meth)acrylates has the potential to become more sustainable than the manufacturing of 1,6-hexanediol diacrylate. The potential for sustainability and the high performance of the biobased furanic monomers make them promising alternatives to petroleum-derived components in sustainable stereolithography resin compositions.

quote

GB/T 7714-2015 [1] Ivan Hevus, Prakash Kannaboina, Yiqiu Qian, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c02207.
MLA [1] Ivan Hevus, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c02207.
APA [1] Ivan Hevus, Prakash Kannaboina, Yiqiu Qian, Jingbo Wu, Melody Johnson, Luke R. Gibbon, John J. La Scala, Chad Ulven, Mukund P. Sibi, & Dean C. Webster. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c02207
IEEE [1] Ivan Hevus, Prakash Kannaboina, Yiqiu Qian, Jingbo Wu, Melody Johnson, Luke R. Gibbon, John J. La Scala, Chad Ulven, Mukund P. Sibi, and Dean C. Webster, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c02207. keywords: {acrylate;methacrylate;biobased monomer;reactive diluent;stereolithography;3D printing;additive manufacturing;BHMF}