Fluorescein-Functionalized Conjugated Polydiacetylenes with Excellent Reversible Thermochromic Properties under Thermal and 980 nm Near-Infrared Light Stimuli AITranslate

Northeast Forestry University; Northeast Forestry University; Northeast Forestry University; Northeast Forestry University; Northeast Forestry University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The design of stimulus-responsive materials with a reversible colorimetric ability is of great value in the applications of sensors, anticounterfeiting, displays, and photodetection. In this article, the chromatic behavior of fluorescein-substituted polydiacetylene (FPDA) was researched in aqueous and solid films. The strong hydrogen bonding and aromatic interactions of the headgroup in FPDA led to an intriguing reversible thermochromism with a green-to-red color transition from 30 to 100 °C in solution and a blue-to-red color transition from 30 to 150 °C in the solid film. The relationships between colorimetric response values and the temperatures indicated the quantitative analysis of the temperature of PDA in both solution and solid films. Furthermore, FPDA displays a reversible color transition from blue to red in response to 980 nm near-infrared light with a higher power light density. Our work may pave the way for broadening the potential applications of PDA-based materials in the field of sensors, display materials, photodetectors, and anticounterfeiting barcode systems.

KeyWords AITranslate

polydiacetylene thermochromism reversibility nearinfrared light selfassemblies
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00862

Chinese Library Classification Number:

Citation Information:

The design of stimulus-responsive materials with a reversible colorimetric ability is of great value in the applications of sensors, anticounterfeiting, displays, and photodetection. In this article, the chromatic behavior of fluorescein-substituted polydiacetylene (FPDA) was researched in aqueous and solid films. The strong hydrogen bonding and aromatic interactions of the headgroup in FPDA led to an intriguing reversible thermochromism with a green-to-red color transition from 30 to 100 °C in solution and a blue-to-red color transition from 30 to 150 °C in the solid film. The relationships between colorimetric response values and the temperatures indicated the quantitative analysis of the temperature of PDA in both solution and solid films. Furthermore, FPDA displays a reversible color transition from blue to red in response to 980 nm near-infrared light with a higher power light density. Our work may pave the way for broadening the potential applications of PDA-based materials in the field of sensors, display materials, photodetectors, and anticounterfeiting barcode systems.

quote

GB/T 7714-2015 [1] Xiaojie Huang, Jie Ji, Guangyao Li, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00862.
MLA [1] Xiaojie Huang, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00862.
APA [1] Xiaojie Huang, Jie Ji, Guangyao Li, Guang Yang, & Juan Hou. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00862