daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Zipping Up NiFe(OH)x-Encapsulated Hematite To Achieve an Ultralow Turn-On Potential for Water Oxidation AITranslate

University of California; University of California; University of California; Sun Yat-sen University; Sun Yat-sen University; Sun Yat-sen University; University of California
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The addition of oxygen evolution reaction (OER) catalysts improves photoelectrochemical (PEC) performance of photoanodes via facilitating charge transfer at the electrode/electrolyte interface and/or passivating surface hole-trap states. Yet, the poor interface and coating quality of the catalyst overlayer often plagues the performance enhancement due to the interference of hole/electron transport across the photoanode/catalyst interface. Here we address these challenges using a citrate-assisted method that allows conformal deposition of Ni–Fe hydroxide [NiFe(OH)x] overlayers on hematite nanowire photoanodes. These NiFe(OH)x overlayers significantly enhance the surface hole transfer kinetics and passivates the surface states. The NiFe(OH)x-encapsulated hematite nanowires exhibit an early turn-on potential of 0.53 V vs RHE. The findings highlight not only the importance of uniform OER catalyst coating but also the critical role of molecular linkers in boosting the performance of photoanodes.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01430

Chinese Library Classification Number:

Citation Information:

The addition of oxygen evolution reaction (OER) catalysts improves photoelectrochemical (PEC) performance of photoanodes via facilitating charge transfer at the electrode/electrolyte interface and/or passivating surface hole-trap states. Yet, the poor interface and coating quality of the catalyst overlayer often plagues the performance enhancement due to the interference of hole/electron transport across the photoanode/catalyst interface. Here we address these challenges using a citrate-assisted method that allows conformal deposition of Ni–Fe hydroxide [NiFe(OH)x] overlayers on hematite nanowire photoanodes. These NiFe(OH)x overlayers significantly enhance the surface hole transfer kinetics and passivates the surface states. The NiFe(OH)x-encapsulated hematite nanowires exhibit an early turn-on potential of 0.53 V vs RHE. The findings highlight not only the importance of uniform OER catalyst coating but also the critical role of molecular linkers in boosting the performance of photoanodes.

quote

GB/T 7714-2015 [1] Mingyang Li, Tianyu Liu, Yi Yang, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01430.
MLA [1] Mingyang Li, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01430.