Composite Hemostat Spray Seals Post-Surgical Blood Burst and Ameliorates Bacteria-Arised Inflammation for Expediting Wound Healing AITranslate

Tongji University; Tongji University; Tongji University; Guangxi Medical University; Guangxi Medical University; Guangxi Medical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Postoperative bleeding and infection are the main causes of death. Although a commercial zeolite-represented hemostatic agent has been widely used, zeolite-induced thermal damages to tissues are unresolved, and antibacterial and wound healing are desirably demanded but challenging. Herein, a composite zeolite-based hemostat spray consisting of Ag-doped β zeolite (Ag-βZ) and coupled fibrinogen/thrombin (F/T) has been developed to seal postsurgical blood burst. Systematic experiments reveal that the F/T can be switched into fibrin gel as the physical barrier and cover Ag-βZ, which imparts the composite hemostats with the most robust hemostasis ability associated with the lowest bleeding amount and the shortest hemostasis time. Concurrently, the physical barrier can shield Ag-βZ from touching water, reduce solvothermal release, and significantly minimize temperature, consequently resulting in no obvious thermal effect on the surrounding tissues. Importantly, the in situ doping of Ag can produce reactive oxygen species to kill bacteria and ameliorate bacteria-aroused inflammation, which can be also leveraged to promote cell expansion for expediting wound healing. The clinically approved components guarantee biosafety, paving a solid foundation for clinical translation.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.3c00212

Chinese Library Classification Number:

Citation Information:

Postoperative bleeding and infection are the main causes of death. Although a commercial zeolite-represented hemostatic agent has been widely used, zeolite-induced thermal damages to tissues are unresolved, and antibacterial and wound healing are desirably demanded but challenging. Herein, a composite zeolite-based hemostat spray consisting of Ag-doped β zeolite (Ag-βZ) and coupled fibrinogen/thrombin (F/T) has been developed to seal postsurgical blood burst. Systematic experiments reveal that the F/T can be switched into fibrin gel as the physical barrier and cover Ag-βZ, which imparts the composite hemostats with the most robust hemostasis ability associated with the lowest bleeding amount and the shortest hemostasis time. Concurrently, the physical barrier can shield Ag-βZ from touching water, reduce solvothermal release, and significantly minimize temperature, consequently resulting in no obvious thermal effect on the surrounding tissues. Importantly, the in situ doping of Ag can produce reactive oxygen species to kill bacteria and ameliorate bacteria-aroused inflammation, which can be also leveraged to promote cell expansion for expediting wound healing. The clinically approved components guarantee biosafety, paving a solid foundation for clinical translation.

quote

GB/T 7714-2015 [1] Tong Xu, Jingwei Hu, Chao Fang, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.3c00212.
MLA [1] Tong Xu, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.3c00212.
APA [1] Tong Xu, Jingwei Hu, Chao Fang, Tao Luo, Junjie Liu, & Kun Zhang. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.3c00212
IEEE [1] Tong Xu, Jingwei Hu, Chao Fang, Tao Luo, Junjie Liu, and Kun Zhang, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.3c00212.