Heterogeneous Electrochemical Ammonia Oxidation with a Ru-bda Oligomer Anchored on Graphitic Electrodes via CH−π Interactions AITranslate
Abstract AITranslate
Molecular catalysts can promote ammonia oxidation, providing mechanistic insights into the electrochemical N2 cycle for a carbon-free fuel economy. We report the ammonia oxidation activity of carbon anodes functionalized with the oligomer {[RuII(bda-κ-N2O2)(4,4′-bpy)]10(4,4′-bpy)}, Rubda-10, where bda is [2,2′-bipyridine]-6,6′-dicarboxylate and 4,4′-bpy is 4,4′-bipyridine. Electrocatalytic studies in propylene carbonate demonstrate that the Ru-based hybrid anode used in a 3-electrode configuration transforms NH3 to N2 and H2 in a 1:3 ratio with near-unity faradaic efficiency at an applied potential of 0.1 V vs Fc+/0, reaching turnover numbers of 7500. X-ray absorption spectroscopic analysis after bulk electrolysis confirms the molecular integrity of the catalyst. Based on computational studies together with electrochemical evidence, ammonia nucleophilic attack is proposed as the primary pathway that leads to critical N–N bond formation.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02483
Chinese Library Classification Number:
Citation Information:
Molecular catalysts can promote ammonia oxidation, providing mechanistic insights into the electrochemical N2 cycle for a carbon-free fuel economy. We report the ammonia oxidation activity of carbon anodes functionalized with the oligomer {[RuII(bda-κ-N2O2)(4,4′-bpy)]10(4,4′-bpy)}, Rubda-10, where bda is [2,2′-bipyridine]-6,6′-dicarboxylate and 4,4′-bpy is 4,4′-bipyridine. Electrocatalytic studies in propylene carbonate demonstrate that the Ru-based hybrid anode used in a 3-electrode configuration transforms NH3 to N2 and H2 in a 1:3 ratio with near-unity faradaic efficiency at an applied potential of 0.1 V vs Fc+/0, reaching turnover numbers of 7500. X-ray absorption spectroscopic analysis after bulk electrolysis confirms the molecular integrity of the catalyst. Based on computational studies together with electrochemical evidence, ammonia nucleophilic attack is proposed as the primary pathway that leads to critical N–N bond formation.
quote
| GB/T 7714-2015 | [1] Anna M. Beiler, Alisa Denisiuk, Jan Holub, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02483. |
| MLA | [1] Anna M. Beiler, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02483. |
| APA | [1] Anna M. Beiler, Alisa Denisiuk, Jan Holub, FranciscoJavier SánchezBaygual, Marcos GilSepulcre, Mehmed Z. Ertem, Dooshaye Moonshiram, Alberto Piccioni, & Antoni Llobet. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02483 |
| IEEE | [1] Anna M. Beiler, Alisa Denisiuk, Jan Holub, FranciscoJavier SánchezBaygual, Marcos GilSepulcre, Mehmed Z. Ertem, Dooshaye Moonshiram, Alberto Piccioni, and Antoni Llobet, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02483. |