daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Oxidative Molecular Layer Deposition of Amine-Containing Conjugated Polymer Thin Films AITranslate

University of Missouri; University of Missouri; University of Missouri; University of Missouri; University of Missouri; University of Missouri
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Conjugated polymers such as polyethylenedioxythiophene (pEDOT), polypyrrole (pPy), and polyaniline (pAni) exhibit high electrochemical capacities, making them appealing as electrode materials for energy storage, electrochemical desalination, and chemical sensing. Recent work has established the growth of thin films of pEDOT using alternating gas-phase exposures of the EDOT monomer and a metal chloride (e.g., MoCl5) oxidant in a process termed oxidative molecular layer deposition (oMLD). Here, we describe the first demonstration of oMLD of amine-containing conjugated polymers. We find that pyrrole (Py) and MoCl5 undergo self-limiting surface reactions during oMLD exposures to form conformal pPy thin films, but oMLD using aniline (Ani) and p-phenylenediamine (PDA) monomers yields unexpected azo functionality. The formation of azo groups is attributed to an MoCl5-amine surface adduct that spatially constrains polymerization reactions near the amine group and produces azo groups when coupling two primary amines. pPy grown by oMLD exhibits a record-breaking 282 mAh/g capacity in an aqueous electrolyte, and PDA/MoCl5 oMLD yields azo polymers of interest as anode materials for alkali-ion batteries. Alternating between Py and PDA monomers during oMLD produces molecularly assembled copolymers with qualitatively different electrochemical responses from the isolated monomer structures. This work lays the foundation for the growth of conformal thin films of conjugated amine polymers with molecular-level control of composition and thickness.

KeyWords AITranslate

nanoscale materials energy storage desalination electrochemistry soft materials
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00942

Chinese Library Classification Number:

Citation Information:

Conjugated polymers such as polyethylenedioxythiophene (pEDOT), polypyrrole (pPy), and polyaniline (pAni) exhibit high electrochemical capacities, making them appealing as electrode materials for energy storage, electrochemical desalination, and chemical sensing. Recent work has established the growth of thin films of pEDOT using alternating gas-phase exposures of the EDOT monomer and a metal chloride (e.g., MoCl5) oxidant in a process termed oxidative molecular layer deposition (oMLD). Here, we describe the first demonstration of oMLD of amine-containing conjugated polymers. We find that pyrrole (Py) and MoCl5 undergo self-limiting surface reactions during oMLD exposures to form conformal pPy thin films, but oMLD using aniline (Ani) and p-phenylenediamine (PDA) monomers yields unexpected azo functionality. The formation of azo groups is attributed to an MoCl5-amine surface adduct that spatially constrains polymerization reactions near the amine group and produces azo groups when coupling two primary amines. pPy grown by oMLD exhibits a record-breaking 282 mAh/g capacity in an aqueous electrolyte, and PDA/MoCl5 oMLD yields azo polymers of interest as anode materials for alkali-ion batteries. Alternating between Py and PDA monomers during oMLD produces molecularly assembled copolymers with qualitatively different electrochemical responses from the isolated monomer structures. This work lays the foundation for the growth of conformal thin films of conjugated amine polymers with molecular-level control of composition and thickness.

quote

GB/T 7714-2015 [1] Quinton K. Wyatt, Mitchel Vaninger, Nikhila C. Paranamana, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00942.
MLA [1] Quinton K. Wyatt, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00942.
APA [1] Quinton K. Wyatt, Mitchel Vaninger, Nikhila C. Paranamana, Thomas W. Heitmann, Helmut Kaiser, & Matthias J. Young. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00942
IEEE [1] Quinton K. Wyatt, Mitchel Vaninger, Nikhila C. Paranamana, Thomas W. Heitmann, Helmut Kaiser, and Matthias J. Young, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00942. keywords: {nanoscale materials;energy storage;desalination;electrochemistry;soft materials}