daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A new approach to characterising the porosity of particle modified electrodes: Potential step chronoamperometry and the diffusion indicator AITranslate

University of Oxford; University of Oxford;MHP Management- und IT-Beratung GmbH, Königsallee 49; University of Oxford
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A new approach is reported for the characterisation of diffusional transport within porous layers used to modify the surfaces of electrodes, as is commonly deployed in the design of new amperometric sensors and for developing electro-catalytic electrodes. In particular we show that measurement and analysis of the current–time transients associated with a potential step at the electrode such that an electroactive analyte is oxidised or reduced at the electrode surface provides much information about the porosity and size of the layer and the constituent particles and highlights the intertwined thin-layer and semi-infinite diffusion as a function of the timescale of electrolysis. The work simulates the chronoamperometry response of electrodes modified with between 0 and 10 layers of spheres acting as partial blocks reducing but not fully preventing diffusional access to the electrode. By analysing the flux-time transient, the diffusion indicator, α , [Le et al., J. Electroanal. Chem, 2019, 855, 113, 602] is shown to be able to reveal bottlenecks to the transport caused by the packing of the spherical blocks and to indicate the timescale at which this is observed which is intermediate to the Cottrellian responses seen at very short or very long times. Further, the indicator provides the point in the flux-time transient at which diffusion is no longer confined to within the porous layer, thus providing a method to estimate the thickness of the porous layer. Graphical abstract Download : Download high-res image (134KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2021.101249

Chinese Library Classification Number:

Citation Information:

A new approach is reported for the characterisation of diffusional transport within porous layers used to modify the surfaces of electrodes, as is commonly deployed in the design of new amperometric sensors and for developing electro-catalytic electrodes. In particular we show that measurement and analysis of the current–time transients associated with a potential step at the electrode such that an electroactive analyte is oxidised or reduced at the electrode surface provides much information about the porosity and size of the layer and the constituent particles and highlights the intertwined thin-layer and semi-infinite diffusion as a function of the timescale of electrolysis. The work simulates the chronoamperometry response of electrodes modified with between 0 and 10 layers of spheres acting as partial blocks reducing but not fully preventing diffusional access to the electrode. By analysing the flux-time transient, the diffusion indicator, α , [Le et al., J. Electroanal. Chem, 2019, 855, 113, 602] is shown to be able to reveal bottlenecks to the transport caused by the packing of the spherical blocks and to indicate the timescale at which this is observed which is intermediate to the Cottrellian responses seen at very short or very long times. Further, the indicator provides the point in the flux-time transient at which diffusion is no longer confined to within the porous layer, thus providing a method to estimate the thickness of the porous layer. Graphical abstract Download : Download high-res image (134KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Minjun Yang, Christopher BatchelorMcAuley, Enno Kätelhön, et al. Applied Materials Today, 2021(25). DOI:10.1016/j.apmt.2021.101249.
MLA [1] Minjun Yang, et al., Applied Materials Today, no. 25, 2021, https://doi.org/10.1016/j.apmt.2021.101249.
APA [1] Minjun Yang, Christopher BatchelorMcAuley, Enno Kätelhön, & Richard G. Compton. (2021). Applied Materials Today(25). https://doi.org/10.1016/j.apmt.2021.101249
IEEE [1] Minjun Yang, Christopher BatchelorMcAuley, Enno Kätelhön, and Richard G. Compton, Applied Materials Today, no. 25, 2021, doi: 10.1016/j.apmt.2021.101249.