Directing Selectivity of Electrochemical Carbon Dioxide Reduction Using Plasmonics AITranslate

University of California; University of California; Lawrence Berkeley National Laboratory; Lawrence Berkeley National Laboratory; Lawrence Berkeley National Laboratory; University of California
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Catalysts for electrochemical carbon dioxide reduction in aqueous electrolytes suffer from high energy input requirements, competition with hydrogen evolution from water reduction, and low product selectivity. Theory suggests that plasmonic catalysts can be tuned to selectively lower the energy barrier for a specific reaction in a set of competitive reactions, but there has been little experimental evidence demonstrating plasmon-driven selectivity in complicated multielectron electrochemical processes. Here, the photoactivity at a plasmonically active silver thin film electrode at small cathodic potentials selectively generates carbon monoxide while simultaneously suppressing hydrogen production. At larger cathodic potentials, the photoactivity promotes production of methanol and formate. Methanol production is observed only under illumination, not in dark conditions. The preference of the plasmonic activity for carbon dioxide reduction over hydrogen evolution and the ability to tune plasmonic activity with voltage demonstrates that plasmonics provide a promising approach to promote complex electrochemical reactions over other competing reactions.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b00515

Chinese Library Classification Number:

Citation Information:

Catalysts for electrochemical carbon dioxide reduction in aqueous electrolytes suffer from high energy input requirements, competition with hydrogen evolution from water reduction, and low product selectivity. Theory suggests that plasmonic catalysts can be tuned to selectively lower the energy barrier for a specific reaction in a set of competitive reactions, but there has been little experimental evidence demonstrating plasmon-driven selectivity in complicated multielectron electrochemical processes. Here, the photoactivity at a plasmonically active silver thin film electrode at small cathodic potentials selectively generates carbon monoxide while simultaneously suppressing hydrogen production. At larger cathodic potentials, the photoactivity promotes production of methanol and formate. Methanol production is observed only under illumination, not in dark conditions. The preference of the plasmonic activity for carbon dioxide reduction over hydrogen evolution and the ability to tune plasmonic activity with voltage demonstrates that plasmonics provide a promising approach to promote complex electrochemical reactions over other competing reactions.

quote

GB/T 7714-2015 [1] Erin B. Creel, Elizabeth R. Corson, Johanna Eichhorn, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00515.
MLA [1] Erin B. Creel, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00515.
APA [1] Erin B. Creel, Elizabeth R. Corson, Johanna Eichhorn, Robert Kostecki, Jeffrey J. Urban, & Bryan D. McCloskey. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00515
IEEE [1] Erin B. Creel, Elizabeth R. Corson, Johanna Eichhorn, Robert Kostecki, Jeffrey J. Urban, and Bryan D. McCloskey, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00515.