α,ω-Bis(trialkoxysilyl) Telechelic Polyolefin/Polyether Copolymers for Adhesive Applications Using Ring-Opening Insertion Metathesis Polymerization Combined with a Chain-Transfer Agent AITranslate
Abstract AITranslate
Monocomponent alkoxysilyl telechelic rigid polyolefins incorporating soft polyether segments along the backbone are valuable adhesives precursors. Herein, the synthesis of α,ω-bis(trialkoxysilyl) telechelic polycyclooctene (PCOE)/poly(propylene glycol31diurethane diacrylate) (PPG*) copolymers is reported from the original combination of Ru-catalyzed ring-opening insertion-metathesis polymerization (ROIMP) with cross metathesis (CM) in the presence of bis(trialkoxysilyl)alkenes as chain-transfer agents (CTAs). The one-pot ROIMP/CM of COE and PPG* diacrylate with {(EtO)3Si(CH2)3NHC(O)OCH2CH═}2 (CTAEt) as the CTA catalyzed by Grubb’s second generation catalyst selectively affords α,ω-[(EtO)3Si]2-PCOE/PPG* copolymers, which show a good thermal stability and a Bingham plastic behavior, as revealed by DSC and rheology. Subsequent curing of the copolymers upon action of moisture with various catalysts unveiled wood-adhesion properties superior to those of commercial silyl-modified polymer (SMP) references.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00311
Chinese Library Classification Number:
Citation Information:
Monocomponent alkoxysilyl telechelic rigid polyolefins incorporating soft polyether segments along the backbone are valuable adhesives precursors. Herein, the synthesis of α,ω-bis(trialkoxysilyl) telechelic polycyclooctene (PCOE)/poly(propylene glycol31diurethane diacrylate) (PPG*) copolymers is reported from the original combination of Ru-catalyzed ring-opening insertion-metathesis polymerization (ROIMP) with cross metathesis (CM) in the presence of bis(trialkoxysilyl)alkenes as chain-transfer agents (CTAs). The one-pot ROIMP/CM of COE and PPG* diacrylate with {(EtO)3Si(CH2)3NHC(O)OCH2CH═}2 (CTAEt) as the CTA catalyzed by Grubb’s second generation catalyst selectively affords α,ω-[(EtO)3Si]2-PCOE/PPG* copolymers, which show a good thermal stability and a Bingham plastic behavior, as revealed by DSC and rheology. Subsequent curing of the copolymers upon action of moisture with various catalysts unveiled wood-adhesion properties superior to those of commercial silyl-modified polymer (SMP) references.
quote
| GB/T 7714-2015 | [1] Cyril Chauveau, Stéphane Fouquay, Guillaume Michaud, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00311. |
| MLA | [1] Cyril Chauveau, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00311. |
| APA | [1] Cyril Chauveau, Stéphane Fouquay, Guillaume Michaud, Frédéric Simon, JeanFrançois Carpentier, & Sophie M. Guillaume. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00311 |
| IEEE | [1] Cyril Chauveau, Stéphane Fouquay, Guillaume Michaud, Frédéric Simon, JeanFrançois Carpentier, and Sophie M. Guillaume, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00311. keywords: {ringopening insertion metathesis polymerization;cross metathesis;chaintransfer agent;alkoxysilyl telechelic;Show More} |