Spiro-Fluorene-Containing Cyclic Olefin Polymers AITranslate

Nagoya Institute of Technology;R&D Enhancement Department, Frontier Materials Laboratories, Osaka Gas Chemicals Co., Ltd.; Nagoya Institute of Technology; Nagoya Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

For application to optical polymer materials with a high refractive index and low birefringence as well as high thermal stability and low hygroscopicity, we have performed the ring-opening metathesis (co)polymerization (ROMP, ROMCP) of fluorene-based norbornene (NB) monomers, spiro[fluorene-9,4′-tricyclo[5.2.1.02,6]dec-8-en] (endo-1 and exo-1) and subsequent hydrogenation to produce spiro-fluorene-containing cyclic olefin polymers. The living ROMP and the kinetics of the ROMCP with NB were investigated. A series of hydrogenated endo- and exo-isomeric polymers, H-poly(1) and H-poly(1-co-NB), with random, gradient, and block sequences, were synthesized and characterized. They are highly soluble in common organic solvents due to their large fractional free volume, as indicated by broad X-ray diffraction patterns. The glass-transition temperatures (Tg) of H-poly(1-co-NB) significantly increased with the content of 1 up to 273 °C [H-poly(endo-1)]. The endo-isomeric polymers exhibited significantly higher Tg values and slightly lower solubility than their exo-counterparts, probably because of the slightly smaller fractional free volume of the endo-isomers. The refractive indexes of H-poly(1)s are as high as 1.61, and the stress-optical coefficients in the rubbery state (CR) of H-poly(1-co-NB) are less than zero. These low birefringences and large fractional free volumes are derived from the bulky spiro-fluorene moiety oriented vertically to the polymer main chain.

KeyWords AITranslate

cyclic olefin polymer fluorene ringopening metathesis polymerization high refractive index low birefringence
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01543

Chinese Library Classification Number:

Citation Information:

For application to optical polymer materials with a high refractive index and low birefringence as well as high thermal stability and low hygroscopicity, we have performed the ring-opening metathesis (co)polymerization (ROMP, ROMCP) of fluorene-based norbornene (NB) monomers, spiro[fluorene-9,4′-tricyclo[5.2.1.02,6]dec-8-en] (endo-1 and exo-1) and subsequent hydrogenation to produce spiro-fluorene-containing cyclic olefin polymers. The living ROMP and the kinetics of the ROMCP with NB were investigated. A series of hydrogenated endo- and exo-isomeric polymers, H-poly(1) and H-poly(1-co-NB), with random, gradient, and block sequences, were synthesized and characterized. They are highly soluble in common organic solvents due to their large fractional free volume, as indicated by broad X-ray diffraction patterns. The glass-transition temperatures (Tg) of H-poly(1-co-NB) significantly increased with the content of 1 up to 273 °C [H-poly(endo-1)]. The endo-isomeric polymers exhibited significantly higher Tg values and slightly lower solubility than their exo-counterparts, probably because of the slightly smaller fractional free volume of the endo-isomers. The refractive indexes of H-poly(1)s are as high as 1.61, and the stress-optical coefficients in the rubbery state (CR) of H-poly(1-co-NB) are less than zero. These low birefringences and large fractional free volumes are derived from the bulky spiro-fluorene moiety oriented vertically to the polymer main chain.

quote

GB/T 7714-2015 [1] Saki Ishii, Yoshiya Ota, Shinichi Matsuoka, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01543.
MLA [1] Saki Ishii, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01543.
APA [1] Saki Ishii, Yoshiya Ota, Shinichi Matsuoka, & Masato Suzuki. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01543
IEEE [1] Saki Ishii, Yoshiya Ota, Shinichi Matsuoka, and Masato Suzuki, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01543. keywords: {cyclic olefin polymer;fluorene;ringopening metathesis polymerization;high refractive index;low birefringence}