Fully Biobased Highly Transparent Nanopaper with UV-Blocking Functionality AITranslate
Abstract AITranslate
The development of green alternatives for petroleum-based plastics is essential for the protection of our environment and its ecosystems. Here, we demonstrate broadband UV-blocking, highly transparent composite nanopaper films from a waste source of cellulose nanofibrils with embedded tunable UV-absorbing nanoparticles (NPs) from ethyl cellulose. These functional nanopaper films are highly transparent, selectively block UV light, and show excellent photostability, therefore with great potential as high-performance, renewable, sustainable, and biodegradable materials for photoprotection applications. Moreover, the integration of functionalized NPs from ethyl cellulose into nanopaper is a platform for novel advanced sustainable materials with a myriad of functionality.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.9b00192
Chinese Library Classification Number:
Citation Information:
The development of green alternatives for petroleum-based plastics is essential for the protection of our environment and its ecosystems. Here, we demonstrate broadband UV-blocking, highly transparent composite nanopaper films from a waste source of cellulose nanofibrils with embedded tunable UV-absorbing nanoparticles (NPs) from ethyl cellulose. These functional nanopaper films are highly transparent, selectively block UV light, and show excellent photostability, therefore with great potential as high-performance, renewable, sustainable, and biodegradable materials for photoprotection applications. Moreover, the integration of functionalized NPs from ethyl cellulose into nanopaper is a platform for novel advanced sustainable materials with a myriad of functionality.
quote
| GB/T 7714-2015 | [1] Douglas R. Hayden, Srivatssan Mohan, Arnout Imhof, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00192. |
| MLA | [1] Douglas R. Hayden, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00192. |
| APA | [1] Douglas R. Hayden, Srivatssan Mohan, Arnout Imhof, & Krassimir P. Velikov. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00192 |
| IEEE | [1] Douglas R. Hayden, Srivatssan Mohan, Arnout Imhof, and Krassimir P. Velikov, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00192. keywords: {biobased;photoprotection;nanopaper;ethyl cellulose nanoparticles;nanocellulose} |