Core-Crosslinked Star Copolymers as Viscosity Index Improvers for Lubricants AITranslate
Abstract AITranslate
Core cross-linked star (CCS) copolymers were prepared by reversible addition–fragmentation chain-transfer polymerization according to the arm-first technique and studied as viscosity index improvers for the application in hydraulic lubricants. A one-pot two-step synthetic procedure was optimized: starting from PMA arms with a precisely controlled structure and three different molecular weights and using different amounts of either divinylbenzene or ethylene glycol dimethacrylate as cross-linking agents, CCS copolymers with a high star yield (63 to 88%) were obtained. CCS copolymers present weight average molecular weight values ranging from 130,000 to 420,000 g mol–1 and a number of arms comprised between 4 and 13. All samples were employed, without any purification step, in the preparation of model lubricant formulations for hydraulic fluid applications. A good compromise between viscosity index improvement and capability to resist chain breaking reactions was obtained for CCS copolymers with target molecular weight for the PMA arms of 20,000 g mol–1. Improved performances with respect to a commercial additive were obtained.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.2c01039
Chinese Library Classification Number:
Citation Information:
Core cross-linked star (CCS) copolymers were prepared by reversible addition–fragmentation chain-transfer polymerization according to the arm-first technique and studied as viscosity index improvers for the application in hydraulic lubricants. A one-pot two-step synthetic procedure was optimized: starting from PMA arms with a precisely controlled structure and three different molecular weights and using different amounts of either divinylbenzene or ethylene glycol dimethacrylate as cross-linking agents, CCS copolymers with a high star yield (63 to 88%) were obtained. CCS copolymers present weight average molecular weight values ranging from 130,000 to 420,000 g mol–1 and a number of arms comprised between 4 and 13. All samples were employed, without any purification step, in the preparation of model lubricant formulations for hydraulic fluid applications. A good compromise between viscosity index improvement and capability to resist chain breaking reactions was obtained for CCS copolymers with target molecular weight for the PMA arms of 20,000 g mol–1. Improved performances with respect to a commercial additive were obtained.
quote
| GB/T 7714-2015 | [1] Katia Sparnacci, Tommaso Frison, Edoardo Podda, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01039. |
| MLA | [1] Katia Sparnacci, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01039. |
| APA | [1] Katia Sparnacci, Tommaso Frison, Edoardo Podda, Diego Antonioli, Michele Laus, Marcello Notari, Giulio Assanelli, Marco Atzeni, Gianfranco Merlini, & Riccardo Pó. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01039 |
| IEEE | [1] Katia Sparnacci, Tommaso Frison, Edoardo Podda, Diego Antonioli, Michele Laus, Marcello Notari, Giulio Assanelli, Marco Atzeni, Gianfranco Merlini, and Riccardo Pó, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01039. keywords: {star copolymers;core crosslinked star copolymers;RAFT polymerization;viscosity index improvers;lubricant additives} |