Covalently Functionalized MoS2 with Dithiolenes AITranslate

Theoretical and Physical Chemistry Institute; CSIC-Universidad de Zaragoza;Theoretical and Physical Chemistry Institute
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Advances are required to develop functionalization routes for MoS2, in both the metallic 1T and semiconducting 2H phase, that will not only enable their easier manipulation and handling in liquid media but also enhance their applicability in diverse technological fields. Herein, we report an original functionalization methodology for covalently incorporating dithiolene units at the periphery of exfoliated 1T- and 2H-MoS2 sheets, by employing a bis(thiolate) salt as a ligand in a green and facile protocol. Extensive characterization of the covalently functionalized materials is presented, along with a pathway for the à la carte chemical manipulation of MoS2. Markedly, the reported methodology may be applied for modifying other transition metal dichalcogenides.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00108

Chinese Library Classification Number:

Citation Information:

Advances are required to develop functionalization routes for MoS2, in both the metallic 1T and semiconducting 2H phase, that will not only enable their easier manipulation and handling in liquid media but also enhance their applicability in diverse technological fields. Herein, we report an original functionalization methodology for covalently incorporating dithiolene units at the periphery of exfoliated 1T- and 2H-MoS2 sheets, by employing a bis(thiolate) salt as a ligand in a green and facile protocol. Extensive characterization of the covalently functionalized materials is presented, along with a pathway for the à la carte chemical manipulation of MoS2. Markedly, the reported methodology may be applied for modifying other transition metal dichalcogenides.

quote

GB/T 7714-2015 [1] Ioanna K. Sideri, Raul Arenal, Nikos Tagmatarchis. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00108.
MLA [1] Ioanna K. Sideri, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00108.
APA [1] Ioanna K. Sideri, Raul Arenal, & Nikos Tagmatarchis. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00108
IEEE [1] Ioanna K. Sideri, Raul Arenal, and Nikos Tagmatarchis, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00108.