daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Polylactic Acid Nanofiber Membranes Grafted with Carbon Nanotubes with Enhanced Mechanical and Electrical Properties AITranslate

Center for Biomaterials and Tissue Engineering. Universitat Politècnica de València. Camino de Vera s/n, Valencia 46022;Center for Biomaterials and Tissue Engineering. Universitat Politècnica de València. Camino de Vera s/n, Valencia 46022;Center for Biomaterials and Tissue Engineering. Universitat Politècnica de València. Camino de Vera s/n, Valencia 46022;Departamento de Termodinámica Aplicada. Universitat Politècnica de València. Camino de Vera s/n, Valencia 46022;Departamento de Termodinámica Aplicada. Universitat Politècnica de València. Camino de Vera s/n, Valencia 46022;Center for Biomaterials and Tissue Engineering. Universitat Politècnica de València. Camino de Vera s/n, Valencia 46022
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Electroconductive materials based on poly(lactic acid) (PLA) electrospinning membranes grafted with carbon nanotubes (CNTs) functionalized with the carboxylic group R–COOH have been obtained. PLA electrospun membranes were modified with sulfuric acid (H2SO4) to oxidize its surface to subsequently graft the CNTs, the treatment time and drying of the membranes before grafting with CNTs being critical, influencing the final properties of the materials. SEM images showed that CNTs presented a uniform distribution on the surface of the PLA nanofibers, while FTIR spectra of PLA-CNTs materials revealed characteristic hydroxyl groups, as evidenced by absorption peaks of CNTs. Thanks to the grafting with CNTs, the resulting PLA-CNTs membranes present an improvement of the mechanical and conductive properties when compared with PLA membranes. On the one hand, grafting with CNTs causes the nanofibers to have greater rigidity, so they are more manipulable and can more easily preserve their conformation when stress is exerted. On the other hand, grafting with CNTs allows elimination of the insulating barrier of the PLA, reducing the resistivity and providing high electrical conductivity to the PLA-CNTs membranes. The incorporation of CNTs into PLA electrospun membranes is expected to offer greater functionalities to electrospun composite nanofibers for medical and industrial applications.

KeyWords AITranslate

polylactic acid carbon nanotubes electrospinning nanofiber membranes grafting
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00776

Chinese Library Classification Number:

Citation Information:

Electroconductive materials based on poly(lactic acid) (PLA) electrospinning membranes grafted with carbon nanotubes (CNTs) functionalized with the carboxylic group R–COOH have been obtained. PLA electrospun membranes were modified with sulfuric acid (H2SO4) to oxidize its surface to subsequently graft the CNTs, the treatment time and drying of the membranes before grafting with CNTs being critical, influencing the final properties of the materials. SEM images showed that CNTs presented a uniform distribution on the surface of the PLA nanofibers, while FTIR spectra of PLA-CNTs materials revealed characteristic hydroxyl groups, as evidenced by absorption peaks of CNTs. Thanks to the grafting with CNTs, the resulting PLA-CNTs membranes present an improvement of the mechanical and conductive properties when compared with PLA membranes. On the one hand, grafting with CNTs causes the nanofibers to have greater rigidity, so they are more manipulable and can more easily preserve their conformation when stress is exerted. On the other hand, grafting with CNTs allows elimination of the insulating barrier of the PLA, reducing the resistivity and providing high electrical conductivity to the PLA-CNTs membranes. The incorporation of CNTs into PLA electrospun membranes is expected to offer greater functionalities to electrospun composite nanofibers for medical and industrial applications.

quote

GB/T 7714-2015 [1] Fernando Gisbert Roca, Cristina MartínezRamos, Sergiy Ivashchenko, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00776.
MLA [1] Fernando Gisbert Roca, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00776.
APA [1] Fernando Gisbert Roca, Cristina MartínezRamos, Sergiy Ivashchenko, Abel GarcíaBernabé, Vicente Compañ, & Manuel Monleón Pradas. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00776
IEEE [1] Fernando Gisbert Roca, Cristina MartínezRamos, Sergiy Ivashchenko, Abel GarcíaBernabé, Vicente Compañ, and Manuel Monleón Pradas, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00776. keywords: {polylactic acid;carbon nanotubes;electrospinning;nanofiber membranes;grafting}