Chitosan-Comodified Surface-Grafted Thermosensitive Ion-Imprinted Composite Membrane for the Selective Recognition and Separation of ReO4– AITranslate

Lanzhou University of Technology; Lanzhou University of Technology; Lanzhou University of Technology; Lanzhou University of Technology; Lanzhou University of Technology; Lanzhou University of Technology; Lanzhou University of Technology; Lanzhou University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With decreasing global rhenium resources, it has become important to separate and purify rhenium in secondary resources, so a preparation strategy for a chitosan-comodified surface-grafted thermosensitive ion-imprinted composite membrane (CS-Re-TIICM) was developed in this work. The key of this design was that the two ends of a poly(N,N-diethylacrylamide) (PDEA) chain were grafted onto the imprinted polymer separating the layer matrix and the surface of the membrane, respectively, which aimed to improve the selectivity and desorption ratio of this material simultaneously. The structure and morphology of this material were characterized by FTIR and SEM, respectively. In addition, CS-Re-TIICM was applied to the secondary leaching solution of the high-temperature alloy to test the actual separation effect, and results showed that CS-Re-TIICM, possessing thermoresponsive recognition sites, and the structure of the imprinting cavity could be adjusted by temperature, which helped this material achieve good selective separation and purification performance for ReO4–. The maximum adsorption capacity was 0.1071 mmol/g at 35 °C. CS-Re-TIICM not only showed an excellent selectivity (separation ReO4–/MnO4– of 3.90 in the presence of interfering ion MnO4–) but also presented an excellent desorption performance (desorption ratio of 68.94%) and good reusability (adsorption capacity of 0.0425 mmol/g, desorption ratio of 59.13%, and separation degree of 1.24). When CS-Re-TIICM was applied to the secondary leaching solution of high-temperature alloys, the purity of Re was increased from 35.41% to 65.10% after one adsorption/desorption cycle, which depicted a prospective application in the industrialized separation of ReO4– from a complex environment.

KeyWords AITranslate

Thermosensitive Imprinted composite membrane ReO4− Selective separation Performance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01169

Chinese Library Classification Number:

Citation Information:

With decreasing global rhenium resources, it has become important to separate and purify rhenium in secondary resources, so a preparation strategy for a chitosan-comodified surface-grafted thermosensitive ion-imprinted composite membrane (CS-Re-TIICM) was developed in this work. The key of this design was that the two ends of a poly(N,N-diethylacrylamide) (PDEA) chain were grafted onto the imprinted polymer separating the layer matrix and the surface of the membrane, respectively, which aimed to improve the selectivity and desorption ratio of this material simultaneously. The structure and morphology of this material were characterized by FTIR and SEM, respectively. In addition, CS-Re-TIICM was applied to the secondary leaching solution of the high-temperature alloy to test the actual separation effect, and results showed that CS-Re-TIICM, possessing thermoresponsive recognition sites, and the structure of the imprinting cavity could be adjusted by temperature, which helped this material achieve good selective separation and purification performance for ReO4–. The maximum adsorption capacity was 0.1071 mmol/g at 35 °C. CS-Re-TIICM not only showed an excellent selectivity (separation ReO4–/MnO4– of 3.90 in the presence of interfering ion MnO4–) but also presented an excellent desorption performance (desorption ratio of 68.94%) and good reusability (adsorption capacity of 0.0425 mmol/g, desorption ratio of 59.13%, and separation degree of 1.24). When CS-Re-TIICM was applied to the secondary leaching solution of high-temperature alloys, the purity of Re was increased from 35.41% to 65.10% after one adsorption/desorption cycle, which depicted a prospective application in the industrialized separation of ReO4– from a complex environment.

quote

GB/T 7714-2015 [1] Xingsheng Liu, Shengyuan Zhao, Wan Xu, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01169.
MLA [1] Xingsheng Liu, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01169.
APA [1] Xingsheng Liu, Shengyuan Zhao, Wan Xu, Huijuan Zhang, Siyuan Lu, Zhenbin Chen, Fangfang Niu, & Gang Wu. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01169
IEEE [1] Xingsheng Liu, Shengyuan Zhao, Wan Xu, Huijuan Zhang, Siyuan Lu, Zhenbin Chen, Fangfang Niu, and Gang Wu, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01169. keywords: {Thermosensitive;Imprinted composite membrane;ReO4−;Selective separation;Performance}