Exploring the Mechanical and Chemical Properties of Cross-Linked Poly(allylamine)-hyaluronic Acid Multilayer Films Using a Chemometric Unmixing Approach AITranslate
Abstract AITranslate
For several decades now, modulating and controlling the mechanical properties of hydrogels, and in particular exponentially growing polyelectrolyte multilayer films (PEMs), have been a major challenge, given their importance in a wide range of applications, including tissue engineering, implantable biomaterials, and drug delivery systems. In this work, we compared the cross-linking reaction of hydrogels based on the association of poly(allylamine) (PAH) and hyaluronic acid (HA) with either 1,4-butanediol diglycidyl ether (BDDE) or divinyl sulfone (DVS) at different concentrations. On the basis of infrared data analysis by means of a chemometric method, we demonstrated that the cross-linking reaction led to significant changes in their chemical features. We deciphered how the affinity of each cross-linker to alcohol and amino chemical functions drives the chemical features of the PEMs. These features can be described by a linear combination of pure HA-BDDE, PAH-BDDE or HA-DVS, and PAH-DVS-based hydrogels with ratios of 80 and 16% for the BDDE and 55 and 45% for the DVS reactions, respectively. Furthermore, the mechanical properties resulting from the BDDE cross-linking reaction were consistent with a high mechanical contribution of HA-BDDE, as estimated by the chemometric analysis. However, this linear combination cannot be applied for DVS. Indeed, the cross-linked PEM was softer than expected, regarding the chemical contributions of HA-DVS and PAH-DVS. Our results show that it is possible to control the mechanical and chemical features by the choice of the cross-linkers alone or in a mixture.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01663
Chinese Library Classification Number:
Citation Information:
For several decades now, modulating and controlling the mechanical properties of hydrogels, and in particular exponentially growing polyelectrolyte multilayer films (PEMs), have been a major challenge, given their importance in a wide range of applications, including tissue engineering, implantable biomaterials, and drug delivery systems. In this work, we compared the cross-linking reaction of hydrogels based on the association of poly(allylamine) (PAH) and hyaluronic acid (HA) with either 1,4-butanediol diglycidyl ether (BDDE) or divinyl sulfone (DVS) at different concentrations. On the basis of infrared data analysis by means of a chemometric method, we demonstrated that the cross-linking reaction led to significant changes in their chemical features. We deciphered how the affinity of each cross-linker to alcohol and amino chemical functions drives the chemical features of the PEMs. These features can be described by a linear combination of pure HA-BDDE, PAH-BDDE or HA-DVS, and PAH-DVS-based hydrogels with ratios of 80 and 16% for the BDDE and 55 and 45% for the DVS reactions, respectively. Furthermore, the mechanical properties resulting from the BDDE cross-linking reaction were consistent with a high mechanical contribution of HA-BDDE, as estimated by the chemometric analysis. However, this linear combination cannot be applied for DVS. Indeed, the cross-linked PEM was softer than expected, regarding the chemical contributions of HA-DVS and PAH-DVS. Our results show that it is possible to control the mechanical and chemical features by the choice of the cross-linkers alone or in a mixture.
quote
| GB/T 7714-2015 | [1] Saeid Ekrami, Fabienne Quilès, Alice Schollhammer, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01663. |
| MLA | [1] Saeid Ekrami, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01663. |
| APA | [1] Saeid Ekrami, Fabienne Quilès, Alice Schollhammer, Xavier Bellanger, Erwan André, & Grégory Francius. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01663 |
| IEEE | [1] Saeid Ekrami, Fabienne Quilès, Alice Schollhammer, Xavier Bellanger, Erwan André, and Grégory Francius, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01663. keywords: {hydrogel;stiffness;atomic force microscopy;crosslinking;infrared spectroscopy} |