Low-Density All-Cellulose Composites Made from Cotton Textile Waste with Promising Thermal Insulation and Acoustic Absorption Properties AITranslate

Mae Fah Luang University; Mae Fah Luang University; Mae Fah Luang University; King Mongkut’s University of Technology Thonburi; Chulalongkorn University; Mae Fah Luang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this study, cotton textile waste (CTW) scraps were used as a starting material to develop low-density all-cellulose composites (ACC–CTWs) via a partial dissolution approach with a NaOH/urea solvent system combined with a vacuum-assisted process. The effect of immersion times on the morphology and characteristics of the resultant ACC–CTWs was examined. These ACC–CTWs exhibited a bulk density of 0.29–0.31 g/cm3. As the immersion time increased, a greater proportion of cellulose I (CTW) was converted to regenerated cellulose (cellulose II). This led to a reduction in its crystallinity. Moreover, the immersion time had a significant effect on the surface and structure of ACC–CTWs, affecting their flexural properties, thermal conductivity, and sound absorption properties. The obtained ACC–CTWs had low thermal conductivity (0.036–0.108 W/mK) and outstanding sound absorption properties, with noise reduction coefficient (NRC) values ranging from 0.68 to 0.83, which are comparable to those of typical building materials. Therefore, the prepared eco-friendly lightweight ACC–CTWs have the potential to serve as effective thermal and acoustic insulation materials in building and construction applications.

KeyWords AITranslate

cotton selfreinforced composites lightweight thermal conductivity sound absorbing material
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02076

Chinese Library Classification Number:

Citation Information:

In this study, cotton textile waste (CTW) scraps were used as a starting material to develop low-density all-cellulose composites (ACC–CTWs) via a partial dissolution approach with a NaOH/urea solvent system combined with a vacuum-assisted process. The effect of immersion times on the morphology and characteristics of the resultant ACC–CTWs was examined. These ACC–CTWs exhibited a bulk density of 0.29–0.31 g/cm3. As the immersion time increased, a greater proportion of cellulose I (CTW) was converted to regenerated cellulose (cellulose II). This led to a reduction in its crystallinity. Moreover, the immersion time had a significant effect on the surface and structure of ACC–CTWs, affecting their flexural properties, thermal conductivity, and sound absorption properties. The obtained ACC–CTWs had low thermal conductivity (0.036–0.108 W/mK) and outstanding sound absorption properties, with noise reduction coefficient (NRC) values ranging from 0.68 to 0.83, which are comparable to those of typical building materials. Therefore, the prepared eco-friendly lightweight ACC–CTWs have the potential to serve as effective thermal and acoustic insulation materials in building and construction applications.

quote

GB/T 7714-2015 [1] Anuphong Suthatho, Phattharasaya Rattanawongkun, Nattaya Tawichai, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02076.
MLA [1] Anuphong Suthatho, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02076.
APA [1] Anuphong Suthatho, Phattharasaya Rattanawongkun, Nattaya Tawichai, Supachok Tanpichai, Anyaporn Boonmahitthisud, & Nattakan Soykeabkaew. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c02076
IEEE [1] Anuphong Suthatho, Phattharasaya Rattanawongkun, Nattaya Tawichai, Supachok Tanpichai, Anyaporn Boonmahitthisud, and Nattakan Soykeabkaew, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c02076. keywords: {cotton;selfreinforced composites;lightweight;thermal conductivity;sound absorbing material}