daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Localized High-Concentration Electrolyte with Optimized Solvents and Lithium Difluoro(oxalate)borate Additive for Stable Lithium Metal Batteries AITranslate

Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Institute of Solid State Physics; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory; Pacific Northwest National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We report a carbonate-based localized high-concentration electrolyte (LHCE) with a fluorinated ether as a diluent for 4-V class lithium metal batteries (LMBs), which enables dendrite-free Li deposition with a high Li Coulombic efficiency (∼98.5%) and much better cycling stability for Li metal anodes than previously reported dimethyl carbonate-based LHCEs at lean electrolyte conditions. This electrolyte consists of 1.2 M lithium bis(fluorosulfonyl)imide (LiFSI) in a cosolvent mixture of ethylene carbonate (EC)/ethyl methyl carbonate (EMC) with bis(2,2,2-trifluoroethyl) ether (BTFE) as the diluent and 0.15 M lithium difluoro(oxalate)borate (LiDFOB) as an additive. A Li||LiNi1/3Mn1/3Co1/3O2 battery with a high areal loading of 3.8 mAh cm–2 maintains 84% of its initial capacity after 100 cycles. The enhanced stability can be attributed to the robust solid–electrolyte interface (SEI) layer formed on the Li metal anode, arising from the preferential decomposition of LiDFOB salt and EC solvent molecules.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b00935

Chinese Library Classification Number:

Citation Information:

We report a carbonate-based localized high-concentration electrolyte (LHCE) with a fluorinated ether as a diluent for 4-V class lithium metal batteries (LMBs), which enables dendrite-free Li deposition with a high Li Coulombic efficiency (∼98.5%) and much better cycling stability for Li metal anodes than previously reported dimethyl carbonate-based LHCEs at lean electrolyte conditions. This electrolyte consists of 1.2 M lithium bis(fluorosulfonyl)imide (LiFSI) in a cosolvent mixture of ethylene carbonate (EC)/ethyl methyl carbonate (EMC) with bis(2,2,2-trifluoroethyl) ether (BTFE) as the diluent and 0.15 M lithium difluoro(oxalate)borate (LiDFOB) as an additive. A Li||LiNi1/3Mn1/3Co1/3O2 battery with a high areal loading of 3.8 mAh cm–2 maintains 84% of its initial capacity after 100 cycles. The enhanced stability can be attributed to the robust solid–electrolyte interface (SEI) layer formed on the Li metal anode, arising from the preferential decomposition of LiDFOB salt and EC solvent molecules.

quote

GB/T 7714-2015 [1] Lu Yu, Shuru Chen, Hongkyung Lee, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b00935.
MLA [1] Lu Yu, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b00935.
APA [1] Lu Yu, Shuru Chen, Hongkyung Lee, Linchao Zhang, Mark H. Engelhard, Qiuyan Li, Shuhong Jiao, Jun Liu, Wu Xu, & JiGuang Zhang. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b00935
IEEE [1] Lu Yu, Shuru Chen, Hongkyung Lee, Linchao Zhang, Mark H. Engelhard, Qiuyan Li, Shuhong Jiao, Jun Liu, Wu Xu, and JiGuang Zhang, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b00935.