NIR-II Dye-Based Multifunctional Telechelic Glycopolymers for NIR-IIa Fluorescence Imaging-Guided Stimuli-Responsive Chemo-Photothermal Combination Therapy AITranslate

Nanjing University of Posts & Telecommunications; Nanjing University of Posts & Telecommunications; Georgia Institute of Technology; Nanjing University of Posts & Telecommunications; Nanjing University of Posts & Telecommunications; Nanjing Tech University (NanjingTech); Liaocheng University; Nanjing University of Posts & Telecommunications; Northwestern Polytechnical University (NPU)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Optical imaging-guided chemo-photothermal combination therapy of cancers has attracted considerable attention, because of its capacity for personalized, precision treatment and its synergistic chemo-photothermal therapeutic effect. However, it still encounters many barriers, including an unsatisfactory diagnostic accuracy, poor physiological stability, low drug loading, and uncontrolled drug release. Here, we developed a NIR-II dye-based multifunctional telechelic glycopolymer (TTQ-TC-PFru) as a drug carrier and constructed stimuli-responsive PFru-BTZ-PBOB nanoparticles (NPs) to achieve the near-infrared IIa (NIR-IIa, 1300-1400 nm) fluorescence imaging (FI)-guided chemo-photothermal combination therapy of cancers. This multifunctional glycopolymer not only serves as the contrast agent for NIR-IIa FI but also functions as the photothermal agent for photothermal therapy (PTT). Meanwhile, the fructose polymer on TTQ-TC-PFru forms a stable boronic acid-catechol conjugate with the dipeptidyl boronic acid proteasome inhibitor bortezomib (BTZ) to achieve high drug loading (31%), satisfactory physiological stability, and controlled drug release in the acidic tumor microenvironment. In addition, one BOB-containing copolymer POEGMA-co-PBOB was introduced to further improve the stability of the system. In living tumor-bearing mice, the successfully constructed stimuli-responsive NPs PFru-BTZ-PBOB induced significant tumor regression through NIR-IIa FI-guided chemo-photothermal combination therapy. Our study thus describes the great potential of NIR-IIa FI-guided chemo-photothermal combination therapy of cancers.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.9b00480

Chinese Library Classification Number:

Citation Information:

Optical imaging-guided chemo-photothermal combination therapy of cancers has attracted considerable attention, because of its capacity for personalized, precision treatment and its synergistic chemo-photothermal therapeutic effect. However, it still encounters many barriers, including an unsatisfactory diagnostic accuracy, poor physiological stability, low drug loading, and uncontrolled drug release. Here, we developed a NIR-II dye-based multifunctional telechelic glycopolymer (TTQ-TC-PFru) as a drug carrier and constructed stimuli-responsive PFru-BTZ-PBOB nanoparticles (NPs) to achieve the near-infrared IIa (NIR-IIa, 1300-1400 nm) fluorescence imaging (FI)-guided chemo-photothermal combination therapy of cancers. This multifunctional glycopolymer not only serves as the contrast agent for NIR-IIa FI but also functions as the photothermal agent for photothermal therapy (PTT). Meanwhile, the fructose polymer on TTQ-TC-PFru forms a stable boronic acid-catechol conjugate with the dipeptidyl boronic acid proteasome inhibitor bortezomib (BTZ) to achieve high drug loading (31%), satisfactory physiological stability, and controlled drug release in the acidic tumor microenvironment. In addition, one BOB-containing copolymer POEGMA-co-PBOB was introduced to further improve the stability of the system. In living tumor-bearing mice, the successfully constructed stimuli-responsive NPs PFru-BTZ-PBOB induced significant tumor regression through NIR-IIa FI-guided chemo-photothermal combination therapy. Our study thus describes the great potential of NIR-IIa FI-guided chemo-photothermal combination therapy of cancers.

quote

GB/T 7714-2015 [1] Shangyu Chen, Bo Sun, Han Miao, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.9b00480.
MLA [1] Shangyu Chen, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.9b00480.
APA [1] Shangyu Chen, Bo Sun, Han Miao, Gaina Wang, Pengfei Sun, Jiewei Li, Wenjun Wang, Quli Fan, & Wei Huang. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.9b00480
IEEE [1] Shangyu Chen, Bo Sun, Han Miao, Gaina Wang, Pengfei Sun, Jiewei Li, Wenjun Wang, Quli Fan, and Wei Huang, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.9b00480.