Iron–Gold Galvanic-Assisted Rapid Grafting of Polymer Brushes on n-Silicon for a Triboelectric Nanogenerator AITranslate

Zhejiang Sci-Tech University; China|University of Chinese Academy of Sciences; Ningbo Institute of Materials Technology and Engineering; China|University of Chinese Academy of Sciences; Zhejiang Sci-Tech University; Ningbo Institute of Materials Technology and Engineering; Ningbo Institute of Materials Technology and Engineering
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The surface-initiated iron(0)-mediated controlled radical polymerization (SI-Fe0CRP) has attracted considerable interest in interface modification because it allows the controlled growth of various polymer brushes on arbitrary substrates under ambient conditions. In order to further expand the polymer brush for different application fields, herein, we propose a robust approach, namely, galvanic-cell-assisted surface-initiated Fe(0)-mediated atom transfer radical polymerization (gc-SI-Fe0ATRP). In gc-SI-Fe0ATRP, an iron-based galvanic cell allows continuous and rapid dissociation of Fe ions in an aqueous environment due to the galvanic-effect-accelerated corrosion of Fe. Through this approach, microliter volumes of various vinyl monomers could be rapidly converted to polymer brushes (up to 864 ± 67 nm in 30 min) with excellent controllability and chain-end fidelity (e.g., the successful preparation of the triblock brushes). We also demonstrate that the gc-SI-Fe0ATRP could efficiently polymerize ionic poly(methacryloyloxy)ethyl trimethylammonium chloride (PMETAC) brushes on large-area n-type silicon for a triboelectric nanogenerator (PB-TENG), which provides an excellent power output of 4.97 μW m–2, more than 11 times higher than the TENG without polymer brush grafted. This work demonstrates an efficient strategy for synthesizing polymer brushes and their potential in the functionalized electrodes for TENGs.

KeyWords AITranslate

gcSIFe0ATRP polymer brushes galvanic cell PMETAC triboelectric nanogenerator
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c02482

Chinese Library Classification Number:

Citation Information:

The surface-initiated iron(0)-mediated controlled radical polymerization (SI-Fe0CRP) has attracted considerable interest in interface modification because it allows the controlled growth of various polymer brushes on arbitrary substrates under ambient conditions. In order to further expand the polymer brush for different application fields, herein, we propose a robust approach, namely, galvanic-cell-assisted surface-initiated Fe(0)-mediated atom transfer radical polymerization (gc-SI-Fe0ATRP). In gc-SI-Fe0ATRP, an iron-based galvanic cell allows continuous and rapid dissociation of Fe ions in an aqueous environment due to the galvanic-effect-accelerated corrosion of Fe. Through this approach, microliter volumes of various vinyl monomers could be rapidly converted to polymer brushes (up to 864 ± 67 nm in 30 min) with excellent controllability and chain-end fidelity (e.g., the successful preparation of the triblock brushes). We also demonstrate that the gc-SI-Fe0ATRP could efficiently polymerize ionic poly(methacryloyloxy)ethyl trimethylammonium chloride (PMETAC) brushes on large-area n-type silicon for a triboelectric nanogenerator (PB-TENG), which provides an excellent power output of 4.97 μW m–2, more than 11 times higher than the TENG without polymer brush grafted. This work demonstrates an efficient strategy for synthesizing polymer brushes and their potential in the functionalized electrodes for TENGs.

quote

GB/T 7714-2015 [1] Shengfei Li, Yuxiang Zhao, Runxiang Tan, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c02482.
MLA [1] Shengfei Li, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c02482.