Modified Cotton Sponge with Bio-Based Polybenzoxazine for Plasticizer Absorption and Oil–Water Separation AITranslate

Yeungnam University; Yeungnam University; Yeungnam University; Yeungnam University; Yeungnam University; Yeungnam University; Yeungnam University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Plastic pollution in the marine environment and oily wastewater generated in industry are now recognized as a real threat, as they adversely affect the environment and cause health issues to living organisms as well. Nevertheless, the current methods for both oil/water separation and plasticizer removal are complex and costly. In this regard, a low-cost and environment-friendly superhydrophobic/superoleophilic material has been developed. Cotton sponge (CS) coated with polybenzoxazine (Pbz) and stearic acid-functionalized carbon balls (CBS) [i.e., CS-Pbz-CBS] acts as a superhydrophobic/oleophilic material. By employing surface modification of CS with Pbz-CBS, the hydrophilic CS gets transformed into superhydrophobic CS-Pbz-CBS possessing a water contact angle of 153°. A surface morphological study indicated the selective wettability produced by CS-Pbz-CBS materials as a result of tuning their surface composition and surface roughness as well. In addition to it, the prepared material CS-Pbz-CBS (6%) also possesses excellent mechanical durability, exhibits fast and efficient separation of oil–water mixtures, and can act as an effective material for plasticizer removal. Moreover, the prepared material, CS-Pbz-CBS (6%), has a volumetric absorption capacity, Qw(v/v), of 83.51 for CHCl3 and provides a 95% separation efficiency for oil/water mixtures. The detailed investigation related to the preparation of these materials and their applicability in oil/water separation and plasticizer removal is analyzed.

KeyWords AITranslate

polybenzoxazine carbon balls cellulose sponge oil/water separation plasticizer removal
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01408

Chinese Library Classification Number:

Citation Information:

Plastic pollution in the marine environment and oily wastewater generated in industry are now recognized as a real threat, as they adversely affect the environment and cause health issues to living organisms as well. Nevertheless, the current methods for both oil/water separation and plasticizer removal are complex and costly. In this regard, a low-cost and environment-friendly superhydrophobic/superoleophilic material has been developed. Cotton sponge (CS) coated with polybenzoxazine (Pbz) and stearic acid-functionalized carbon balls (CBS) [i.e., CS-Pbz-CBS] acts as a superhydrophobic/oleophilic material. By employing surface modification of CS with Pbz-CBS, the hydrophilic CS gets transformed into superhydrophobic CS-Pbz-CBS possessing a water contact angle of 153°. A surface morphological study indicated the selective wettability produced by CS-Pbz-CBS materials as a result of tuning their surface composition and surface roughness as well. In addition to it, the prepared material CS-Pbz-CBS (6%) also possesses excellent mechanical durability, exhibits fast and efficient separation of oil–water mixtures, and can act as an effective material for plasticizer removal. Moreover, the prepared material, CS-Pbz-CBS (6%), has a volumetric absorption capacity, Qw(v/v), of 83.51 for CHCl3 and provides a 95% separation efficiency for oil/water mixtures. The detailed investigation related to the preparation of these materials and their applicability in oil/water separation and plasticizer removal is analyzed.

quote

GB/T 7714-2015 [1] Thirukumaran Periyasamy, Shakila Parveen Asrafali, Rajesh Haldhar, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01408.
MLA [1] Thirukumaran Periyasamy, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01408.
APA [1] Thirukumaran Periyasamy, Shakila Parveen Asrafali, Rajesh Haldhar, Santhamoorthy Madhappan, Ramkumar Vanaraj, Chaitany Jayprakash Raorane, & SeongCheol Kim. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01408
IEEE [1] Thirukumaran Periyasamy, Shakila Parveen Asrafali, Rajesh Haldhar, Santhamoorthy Madhappan, Ramkumar Vanaraj, Chaitany Jayprakash Raorane, and SeongCheol Kim, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01408. keywords: {polybenzoxazine;carbon balls;cellulose sponge;oil/water separation;plasticizer removal}