daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Super Atmospheric Water Harvesting Hydrogel with Alginate Chains Modified with Binary Salts AITranslate

Shanghai Jiao Tong University; Shanghai Jiao Tong University; Shanghai Jiao Tong University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Atmospheric water harvesting is considered to be a promising technology to address the global water shortage. However, researchers are still searching for optimized desiccants with all of the desired features, such as high water sorption capacity, low desorption temperature, wide light spectrum absorption, ease to scale up, and low cost. Here, we modified sodium alginate by occupying both G-blocks and M-blocks with more hydrophilic cations (i.e., Li and Ca). Functionalized carbon nanotubes (FCNTs) are embedded in the hydrogel structure to increase solar spectrum absorption. In summary, these features enable binary composite to adsorb ∼5.6 g of water per gram of desiccant. For the first time, the idea of rational combination of a binary hydrophilic polymeric salt was embodied. We believe that this binary/FCNT sorbent is a promising material for application in water sorption-based technologies.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.9b00315

Chinese Library Classification Number:

Citation Information:

Atmospheric water harvesting is considered to be a promising technology to address the global water shortage. However, researchers are still searching for optimized desiccants with all of the desired features, such as high water sorption capacity, low desorption temperature, wide light spectrum absorption, ease to scale up, and low cost. Here, we modified sodium alginate by occupying both G-blocks and M-blocks with more hydrophilic cations (i.e., Li and Ca). Functionalized carbon nanotubes (FCNTs) are embedded in the hydrogel structure to increase solar spectrum absorption. In summary, these features enable binary composite to adsorb ∼5.6 g of water per gram of desiccant. For the first time, the idea of rational combination of a binary hydrophilic polymeric salt was embodied. We believe that this binary/FCNT sorbent is a promising material for application in water sorption-based technologies.

quote

GB/T 7714-2015 [1] Akram Entezari, Mojtaba Ejeian, Ruzhu Wang. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.9b00315.
MLA [1] Akram Entezari, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.9b00315.
APA [1] Akram Entezari, Mojtaba Ejeian, & Ruzhu Wang. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.9b00315
IEEE [1] Akram Entezari, Mojtaba Ejeian, and Ruzhu Wang, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.9b00315.