daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on 3D-Printed Emodin/Nano-Hydroxyapatite Scaffolds Promoting Bone Regeneration by Supporting Osteoblast Proliferation and Macrophage M2 Polarization AITranslate

Nanjing Medical University; Nanjing Medical University; Nanjing Medical University; Nanjing Medical University; Nanjing Medical University; Changzhou University; Nanjing Medical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The treatment of bone defects caused by diseases, trauma, or tumor has always been a great clinical challenge. Implantation of bone biomaterials into bone defect areas is an effective method for bone injury repair. In this study, we used three-dimensional (3D) printing technology to prepare nano-hydroxyapatite (nHA)/sodium alginate (SA)/gelatin (Gel) hydrogel scaffolds loaded with different ratios (0, 0.13, 0.26, 0.39, 0.53, and 0.79‰) of emodin (EM) (EM/nHA/SA/Gel). Scanning electron microscopy showed that the scaffolds had a smooth surface without fracture and nHA was evenly distributed on the surface. The cell proliferation and migration results showed that the 0.39‰ EM group, in particular, could significantly promote the proliferation and migration of mouse embryonic osteoblast precursor (MC3T3-E1) cells and significantly increase the mRNA expression of osteogenic differentiation-related genes (bone morphogenetic protein/BMP-2, BMP-9, osteocalcin). In addition, the 0.39‰ EM group exhibited the best effect on osteogenic differentiation-related proteins (alkaline phosphatase, Runx 2, OSX). The expression of M2 polarization-related genes (arginase-1, CD206) also significantly increased after the treatment with the 0.39‰ EM group. Micro-CT showed that in the rat skull defect model, the EM/nHA/SA/Gel scaffold group significantly promoted bone regeneration after being implanted into the skull for 30 days. Our results indicate that the EM/nHA/SA/Gel hydrogel scaffolds can not only directly promote the proliferation and differentiation of osteoblasts but also indirectly promote osteogenic differentiation by supporting M2 polarization of macrophages. EM/nHA/SA/Gel hydrogel scaffolds are potential bone tissue engineering materials for bone regeneration.

KeyWords AITranslate

emodin bone regeneration 3D printing osteogenesis immunity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00296

Chinese Library Classification Number:

Citation Information:

The treatment of bone defects caused by diseases, trauma, or tumor has always been a great clinical challenge. Implantation of bone biomaterials into bone defect areas is an effective method for bone injury repair. In this study, we used three-dimensional (3D) printing technology to prepare nano-hydroxyapatite (nHA)/sodium alginate (SA)/gelatin (Gel) hydrogel scaffolds loaded with different ratios (0, 0.13, 0.26, 0.39, 0.53, and 0.79‰) of emodin (EM) (EM/nHA/SA/Gel). Scanning electron microscopy showed that the scaffolds had a smooth surface without fracture and nHA was evenly distributed on the surface. The cell proliferation and migration results showed that the 0.39‰ EM group, in particular, could significantly promote the proliferation and migration of mouse embryonic osteoblast precursor (MC3T3-E1) cells and significantly increase the mRNA expression of osteogenic differentiation-related genes (bone morphogenetic protein/BMP-2, BMP-9, osteocalcin). In addition, the 0.39‰ EM group exhibited the best effect on osteogenic differentiation-related proteins (alkaline phosphatase, Runx 2, OSX). The expression of M2 polarization-related genes (arginase-1, CD206) also significantly increased after the treatment with the 0.39‰ EM group. Micro-CT showed that in the rat skull defect model, the EM/nHA/SA/Gel scaffold group significantly promoted bone regeneration after being implanted into the skull for 30 days. Our results indicate that the EM/nHA/SA/Gel hydrogel scaffolds can not only directly promote the proliferation and differentiation of osteoblasts but also indirectly promote osteogenic differentiation by supporting M2 polarization of macrophages. EM/nHA/SA/Gel hydrogel scaffolds are potential bone tissue engineering materials for bone regeneration.

quote

GB/T 7714-2015 [1] Yiwen Pan, Shaoqing Chen, Yanyan Meng, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00296.
MLA [1] Yiwen Pan, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00296.
APA [1] Yiwen Pan, Shaoqing Chen, Yanyan Meng, Mu He, Chun Liu, Cheli Wang, & Xinye Ni. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00296
IEEE [1] Yiwen Pan, Shaoqing Chen, Yanyan Meng, Mu He, Chun Liu, Cheli Wang, and Xinye Ni, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00296. keywords: {emodin;bone regeneration;3D printing;osteogenesis;immunity}