Control in Coloration and Estimation of the Refractive Index by Porous Polymeric Membranes Prepared by the “Miniemulsion” Templating Method AITranslate

Keio University; Keio University; Keio University; Keio University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

We fabricated porous polymeric membranes using the miniemulsion templating method to investigate the transmitted and scattered lights in terms of the Christiansen filter effect. This method made it possible to produce porous polymeric membranes with different refractive indices by polymerization of different monomers and copolymerization of monomers. When a membrane with an open-cellular structure was immersed in a liquid, the transmitted light was observed at a wavelength where the refractive indices of the polymeric phase and the liquid matched. Angle-independent color derived from the scattered light could also be observed. When the porous membrane of poly(2-ethylhexyl methacrylate) (EHMA) was immersed in a mixture of different kinds of liquids, the maximum wavelength of the transmission (λmax) changed according to the refractive index matching of the polymeric phase and the liquid, resulting in the change in coloration. Next, when the P(EHMA-co-EGDMA) membrane was immersed in a mixture of toluene and d-limonene, λmax and color varied depending on their mixing ratios. This coloration was controlled by temperature and the refractive indices of the polymeric phase and the liquid. Furthermore, we could estimate the refractive index of PEGDMA using λmax values obtained by immersing it into liquids with different refractive indices.

KeyWords AITranslate

miniemulsion porous membranes structural colors Christiansen filter effect refractive index
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01230

Chinese Library Classification Number:

Citation Information:

We fabricated porous polymeric membranes using the miniemulsion templating method to investigate the transmitted and scattered lights in terms of the Christiansen filter effect. This method made it possible to produce porous polymeric membranes with different refractive indices by polymerization of different monomers and copolymerization of monomers. When a membrane with an open-cellular structure was immersed in a liquid, the transmitted light was observed at a wavelength where the refractive indices of the polymeric phase and the liquid matched. Angle-independent color derived from the scattered light could also be observed. When the porous membrane of poly(2-ethylhexyl methacrylate) (EHMA) was immersed in a mixture of different kinds of liquids, the maximum wavelength of the transmission (λmax) changed according to the refractive index matching of the polymeric phase and the liquid, resulting in the change in coloration. Next, when the P(EHMA-co-EGDMA) membrane was immersed in a mixture of toluene and d-limonene, λmax and color varied depending on their mixing ratios. This coloration was controlled by temperature and the refractive indices of the polymeric phase and the liquid. Furthermore, we could estimate the refractive index of PEGDMA using λmax values obtained by immersing it into liquids with different refractive indices.

quote

GB/T 7714-2015 [1] Yuuka Fukui, Haruna Sumida, Yusuke Sugaya, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01230.
MLA [1] Yuuka Fukui, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01230.
APA [1] Yuuka Fukui, Haruna Sumida, Yusuke Sugaya, & Keiji Fujimoto. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01230
IEEE [1] Yuuka Fukui, Haruna Sumida, Yusuke Sugaya, and Keiji Fujimoto, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01230. keywords: {miniemulsion;porous membranes;structural colors;Christiansen filter effect;refractive index}