Abstract AITranslate

In this work, biocompatible composite fibers were prepared from human hair keratin and plant cellulose with different proportions by the wet-spinning method, and their properties and performance, including chemical structures, morphology, mechanical strength, and cell proliferation and attachment, were systematically investigated. It showed that the best proportion of the keratin/cellulose mass ratio was 30:70, and its tensile strength reached 277 MPa (elongation at break can be 27%), which is higher than that of the regenerated cellulose fiber (193 MPa, 12%). Its viability and proliferation of L929 murine fibroblast cells are also better than those of the regenerated cellulose fiber. Atomistic simulations were carried out and demonstrated the formation of hydrogen bonds between keratin and cellulose molecules, clarifying that the ratio of keratin has a significant effect on the aggregation structures in the solution and that the hydrogen bonds formed between keratin and cellulose molecules have a distinct contribution to the biocompatible composites. This work demonstrates the potential of the prepared composite fiber in biomedical applications and provides an innovative way to utilize waste human hair as a high-value raw material.

KeyWords AITranslate

ionic liquids keratin composite fiber biocompatible molecular dynamics simulation
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01912

Chinese Library Classification Number:

Citation Information:

In this work, biocompatible composite fibers were prepared from human hair keratin and plant cellulose with different proportions by the wet-spinning method, and their properties and performance, including chemical structures, morphology, mechanical strength, and cell proliferation and attachment, were systematically investigated. It showed that the best proportion of the keratin/cellulose mass ratio was 30:70, and its tensile strength reached 277 MPa (elongation at break can be 27%), which is higher than that of the regenerated cellulose fiber (193 MPa, 12%). Its viability and proliferation of L929 murine fibroblast cells are also better than those of the regenerated cellulose fiber. Atomistic simulations were carried out and demonstrated the formation of hydrogen bonds between keratin and cellulose molecules, clarifying that the ratio of keratin has a significant effect on the aggregation structures in the solution and that the hydrogen bonds formed between keratin and cellulose molecules have a distinct contribution to the biocompatible composites. This work demonstrates the potential of the prepared composite fiber in biomedical applications and provides an innovative way to utilize waste human hair as a high-value raw material.

quote

GB/T 7714-2015 [1] Congwen Qin, Yonglei Wang, Hongshuai Gao, et al. ACS Applied Polymer Materials, 2024(6). DOI:10.1021/acsapm.3c01912.
MLA [1] Congwen Qin, et al., ACS Applied Polymer Materials, no. 6, 2024, https://doi.org/10.1021/acsapm.3c01912.
APA [1] Congwen Qin, Yonglei Wang, Hongshuai Gao, Xue Liu, Yi Nie, & Xiaoyan Ji. (2024). ACS Applied Polymer Materials(6). https://doi.org/10.1021/acsapm.3c01912
IEEE [1] Congwen Qin, Yonglei Wang, Hongshuai Gao, Xue Liu, Yi Nie, and Xiaoyan Ji, ACS Applied Polymer Materials, no. 6, 2024, doi: 10.1021/acsapm.3c01912. keywords: {ionic liquids;keratin;composite fiber;biocompatible;molecular dynamics simulation}