Pressure-Induced Emission Enhancements of Mn2+-Doped Cesium Lead Chloride Perovskite Nanocrystals AITranslate

Jilin University; Jilin University; Dalian Institute of Chemical Physics; Jilin University; Jilin University; Jilin University; Jilin University; Dalian Institute of Chemical Physics; Dalian Institute of Chemical Physics; Jilin University; Zhengzhou University; Jilin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Metal-halide perovskites (MHPs) have attracted tremendous attention because of their excellent performance in photovoltaic devices, such as solar cells. However, because of the crucial relationship between emission intensity and performance, pressure-quenching of optical emission greatly restrict the potential application of MHPs. Here, we reported the unique pressure-induced emission enhancement (PIEE) of CsPbxMn1–xCl3 NCs. Different from other PIEE phenomena, the PIEE of CsPbxMn1–xCl3 NCs was caused by the enhancement of energy release from 4T1 to 6A1 of the Mn, attributed to the pressure-induced isostructural phase transition. Meanwhile, the photoluminescence (PL) can exist until almost 20 GPa, suggesting that CsPbxMn1–xCl3 NCs exhibited better environmental suitability and worked under high pressure. Our studies explored the relationship between bandgap microstructure and optical properties of CsPbxMn1–xCl3 NCs at high pressure and also gave insights into the optimization of photovoltaic performance, which promoting the design of functional MHPs.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.0c00033

Chinese Library Classification Number:

Citation Information:

Metal-halide perovskites (MHPs) have attracted tremendous attention because of their excellent performance in photovoltaic devices, such as solar cells. However, because of the crucial relationship between emission intensity and performance, pressure-quenching of optical emission greatly restrict the potential application of MHPs. Here, we reported the unique pressure-induced emission enhancement (PIEE) of CsPbxMn1–xCl3 NCs. Different from other PIEE phenomena, the PIEE of CsPbxMn1–xCl3 NCs was caused by the enhancement of energy release from 4T1 to 6A1 of the Mn, attributed to the pressure-induced isostructural phase transition. Meanwhile, the photoluminescence (PL) can exist until almost 20 GPa, suggesting that CsPbxMn1–xCl3 NCs exhibited better environmental suitability and worked under high pressure. Our studies explored the relationship between bandgap microstructure and optical properties of CsPbxMn1–xCl3 NCs at high pressure and also gave insights into the optimization of photovoltaic performance, which promoting the design of functional MHPs.

quote

GB/T 7714-2015 [1] Ye Cao, Guangyu Qi, Laizhi Sui, et al. ACS Materials Letters, 2020(2). DOI:10.1021/acsmaterialslett.0c00033.
MLA [1] Ye Cao, et al., ACS Materials Letters, no. 2, 2020, https://doi.org/10.1021/acsmaterialslett.0c00033.
APA [1] Ye Cao, Guangyu Qi, Laizhi Sui, Yue Shi, Ting Geng, Dianlong Zhao, Kai Wang, Kaijun Yuan, Guorong Wu, Guanjun Xiao, Siyu Lu, & Bo Zou. (2020). ACS Materials Letters(2). https://doi.org/10.1021/acsmaterialslett.0c00033
IEEE [1] Ye Cao, Guangyu Qi, Laizhi Sui, Yue Shi, Ting Geng, Dianlong Zhao, Kai Wang, Kaijun Yuan, Guorong Wu, Guanjun Xiao, Siyu Lu, and Bo Zou, ACS Materials Letters, no. 2, 2020, doi: 10.1021/acsmaterialslett.0c00033.