The crystal structures of some RM and RM2 compounds (where R=rare earth metal and M=non - rare earth metal) AITranslate
Abstract AITranslate
The non-cubic crystal structures of YIn, YPd and YAu are reported for the first time. YIn has the disordered tetragonal L10 CuAu-type structure, and both YPd and YAu are isostructural with the orthorhombic B33 CrB -type structure. The lattice parameters for some C15 MgCu2-type Laves phase (TbxDy1−x)Al2 alloys ( x = 0.25 , 0.50 , 0.75 and 1.0) have been measured and are found to vary linearly with composition between x = 0.25 and 1.0.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.calphad.2008.07.008
Chinese Library Classification Number:
Citation Information:
The non-cubic crystal structures of YIn, YPd and YAu are reported for the first time. YIn has the disordered tetragonal L10 CuAu-type structure, and both YPd and YAu are isostructural with the orthorhombic B33 CrB -type structure. The lattice parameters for some C15 MgCu2-type Laves phase (TbxDy1−x)Al2 alloys ( x = 0.25 , 0.50 , 0.75 and 1.0) have been measured and are found to vary linearly with composition between x = 0.25 and 1.0.
quote
| GB/T 7714-2015 | [1] K.A. Gschneidner, Ya. Mudryk, A.T. Becker, et al. Calphad, 2009(33). DOI:10.1016/j.calphad.2008.07.008. |
| MLA | [1] K.A. Gschneidner, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2008.07.008. |
| APA | [1] K.A. Gschneidner, Ya. Mudryk, A.T. Becker, & J.L. Larson. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2008.07.008 |