Coadditive Engineering with 5-Ammonium Valeric Acid Iodide for Efficient and Stable Sn Perovskite Solar Cells AITranslate

University of Tsukuba; University of Tsukuba; National Institute for Materials Science (NIMS); National Institute of Advanced Industrial Science and Technology (AIST); Dongguk University; National Institute for Materials Science (NIMS); National Institute for Materials Science (NIMS)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Sn-based perovskite solar cells (PSCs) featuring high performance and long-term stability are very challenging because Sn2+ is relatively prone to oxidation. Here, we have performed coadditive engineering with 5-ammonium valeric acid iodide (5-AVAI) for FASnI3-based perovskite films. From the morphological, structural, and elemental analyses, we observed that 5-AVAI affects the crystal growth of perovskites through its hydrogen bond with I– of the SnI64– octahedral. As a result, pinhole-free homogeneous and stable Sn-based perovskite films form over a large area with lower Sn4+ content. This made us able to enhance the power conversion efficiency (PCE) for Sn-based PSCs up to 7% in a 0.25 cm2 aperture area. Most importantly, the 5-AVAI added PSCs showed a record stability and maintained their initial PCE under 1 sun continuous illumination at maximum power point tracking for 100 h.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b02216

Chinese Library Classification Number:

Citation Information:

Sn-based perovskite solar cells (PSCs) featuring high performance and long-term stability are very challenging because Sn2+ is relatively prone to oxidation. Here, we have performed coadditive engineering with 5-ammonium valeric acid iodide (5-AVAI) for FASnI3-based perovskite films. From the morphological, structural, and elemental analyses, we observed that 5-AVAI affects the crystal growth of perovskites through its hydrogen bond with I– of the SnI64– octahedral. As a result, pinhole-free homogeneous and stable Sn-based perovskite films form over a large area with lower Sn4+ content. This made us able to enhance the power conversion efficiency (PCE) for Sn-based PSCs up to 7% in a 0.25 cm2 aperture area. Most importantly, the 5-AVAI added PSCs showed a record stability and maintained their initial PCE under 1 sun continuous illumination at maximum power point tracking for 100 h.

quote

GB/T 7714-2015 [1] Md. Emrul Kayesh, Kiyoto Matsuishi, Ryuji Kaneko, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b02216.
MLA [1] Md. Emrul Kayesh, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b02216.
APA [1] Md. Emrul Kayesh, Kiyoto Matsuishi, Ryuji Kaneko, Said Kazaoui, JaeJoon Lee, Takeshi Noda, & Ashraful Islam. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b02216
IEEE [1] Md. Emrul Kayesh, Kiyoto Matsuishi, Ryuji Kaneko, Said Kazaoui, JaeJoon Lee, Takeshi Noda, and Ashraful Islam, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b02216.