daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Ab initio calculation of the BCC Fe–Al–Mo (Iron–Aluminum–Molybdenum) phase diagram: Implications for the nature of the τ 2 phase AITranslate

Instituto de Fìsica da Universidade de São Paulo; Universidad Nacional del Callao; Instituto de Fìsica da Universidade de São Paulo; Escola Politécnica da Universidade de São Paulo
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The metastable phase diagram of the BCC-based ordering equilibria in the Fe–Al–Mo system has been calculated via a truncated cluster expansion, through the combination of Full-Potential-Linear augmented Plane Wave (FP-LAPW) electronic structure calculations and of Cluster Variation Method (CVM) thermodynamic calculations in the irregular tetrahedron approximation. Four isothermal sections at 1750 K, 2000 K, 2250 K and 2500 K are calculated and correlated with recently published experimental data on the system. The results confirm that the critical temperature for the order–disorder equilibrium between Fe3Al–D03 and FeAl–B2 is increased by Mo additions, while the critical temperature for the FeAl–B2/A2 equilibrium is kept approximately invariant with increasing Mo contents. The stabilization of the Al-rich A2 phase in equilibrium with overstoichiometric B2–(Fe,Mo)Al is also consistent with the attribution of the A2 structure to the τ 2 phase, stable at high temperatures in overstoichiometric B2–FeAl.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2009.04.003

Chinese Library Classification Number:

Citation Information:

The metastable phase diagram of the BCC-based ordering equilibria in the Fe–Al–Mo system has been calculated via a truncated cluster expansion, through the combination of Full-Potential-Linear augmented Plane Wave (FP-LAPW) electronic structure calculations and of Cluster Variation Method (CVM) thermodynamic calculations in the irregular tetrahedron approximation. Four isothermal sections at 1750 K, 2000 K, 2250 K and 2500 K are calculated and correlated with recently published experimental data on the system. The results confirm that the critical temperature for the order–disorder equilibrium between Fe3Al–D03 and FeAl–B2 is increased by Mo additions, while the critical temperature for the FeAl–B2/A2 equilibrium is kept approximately invariant with increasing Mo contents. The stabilization of the Al-rich A2 phase in equilibrium with overstoichiometric B2–(Fe,Mo)Al is also consistent with the attribution of the A2 structure to the τ 2 phase, stable at high temperatures in overstoichiometric B2–FeAl.

quote

GB/T 7714-2015 [1] Ney Sodré, Pablo Guillermo GonzalesOrmeño, Helena Maria Petrilli, et al. Calphad, 2009(33). DOI:10.1016/j.calphad.2009.04.003.
MLA [1] Ney Sodré, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2009.04.003.
APA [1] Ney Sodré, Pablo Guillermo GonzalesOrmeño, Helena Maria Petrilli, & Cláudio Geraldo Schön. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2009.04.003
IEEE [1] Ney Sodré, Pablo Guillermo GonzalesOrmeño, Helena Maria Petrilli, and Cláudio Geraldo Schön, Calphad, no. 33, 2009, doi: 10.1016/j.calphad.2009.04.003.