Atomic mobilities, uphill diffusion and proeutectic ferrite growth in Fe–Mn–C alloys AITranslate

Montana State University; Central South University; Central South University;American Water Chemicals Inc.;DNV Columbus
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Following the treatment in CALPHAD, experimental data on diffusivities in Fe–Mn and Fe–C binary systems are critically evaluated with the DICTRA software to derive atomic mobilities. The effect of magnetic ordering on diffusion in bcc phase is taken into account, and the obtained atomic mobilities are expressed as functions of temperature and compositions with the Redlick–Kister polynomials. Based on the mobility parameters obtained in this work for the end-members and the interaction terms, comprehensive comparisons between the calculated and experimentally measured quantities are made. Due to the lack of experimental diffusivities for the ternary system, extrapolation based on binary information is performed, the results of which are used to study uphill diffusion of C in fcc Fe–Mn–C alloys. Such C diffusion against its own concentration gradient is a common occurrence for ternary systems containing one interstitial element, provided that the initial alloy compositions of diffusion couples are well chosen. In addition, the operating tie line evolution for proeutectic ferrite growth is also investigated, where C diffusion-controlled fast and Mn diffusion-controlled slow growths are discussed.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2009.07.002

Chinese Library Classification Number:

Citation Information:

Following the treatment in CALPHAD, experimental data on diffusivities in Fe–Mn and Fe–C binary systems are critically evaluated with the DICTRA software to derive atomic mobilities. The effect of magnetic ordering on diffusion in bcc phase is taken into account, and the obtained atomic mobilities are expressed as functions of temperature and compositions with the Redlick–Kister polynomials. Based on the mobility parameters obtained in this work for the end-members and the interaction terms, comprehensive comparisons between the calculated and experimentally measured quantities are made. Due to the lack of experimental diffusivities for the ternary system, extrapolation based on binary information is performed, the results of which are used to study uphill diffusion of C in fcc Fe–Mn–C alloys. Such C diffusion against its own concentration gradient is a common occurrence for ternary systems containing one interstitial element, provided that the initial alloy compositions of diffusion couples are well chosen. In addition, the operating tie line evolution for proeutectic ferrite growth is also investigated, where C diffusion-controlled fast and Mn diffusion-controlled slow growths are discussed.

quote

GB/T 7714-2015 [1] Yajun Liu, Lijun Zhang, Yong Du, et al. Calphad, 2009(33). DOI:10.1016/j.calphad.2009.07.002.
MLA [1] Yajun Liu, et al., Calphad, no. 33, 2009, https://doi.org/10.1016/j.calphad.2009.07.002.
APA [1] Yajun Liu, Lijun Zhang, Yong Du, Di Yu, & Dong Liang. (2009). Calphad(33). https://doi.org/10.1016/j.calphad.2009.07.002
IEEE [1] Yajun Liu, Lijun Zhang, Yong Du, Di Yu, and Dong Liang, Calphad, no. 33, 2009, doi: 10.1016/j.calphad.2009.07.002.