daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Regulating Electrocatalysts via Surface and Interface Engineering for Acidic Water Electrooxidation AITranslate

The University of Adelaide; The University of Adelaide; Henan University; The University of Adelaide; The University of Adelaide
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Although proton exchange membrane (PEM) water electrolyzers offer a promising means for generation of hydrogen fuel from solar and wind energy, in acidic environments the corresponding anodic oxygen evolution reaction (OER) remains a bottleneck. Because the activity and stability of electrocatalysts depend significantly on physicochemical properties, material surface and interface engineering can offer a practical way to boost performance. To date, significant advances have been made using a judicious combination of advanced theoretical computations and spectroscopic characterizations. To provide a critical assessment of this field, we focus on the establishment of material property–catalytic activity relationships. We start with a detailed exploration of prevailing OER mechanisms in acid solution through evaluating the role of catalyst lattice oxygen. We then critically review advances in surface and interface engineering in acidic OER electrocatalysts from both experimental and theoretical perspectives. Finally, a few promising research orientations are proposed to inspire future investigation of high-performance PEM catalysts.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.9b01758

Chinese Library Classification Number:

Citation Information:

Although proton exchange membrane (PEM) water electrolyzers offer a promising means for generation of hydrogen fuel from solar and wind energy, in acidic environments the corresponding anodic oxygen evolution reaction (OER) remains a bottleneck. Because the activity and stability of electrocatalysts depend significantly on physicochemical properties, material surface and interface engineering can offer a practical way to boost performance. To date, significant advances have been made using a judicious combination of advanced theoretical computations and spectroscopic characterizations. To provide a critical assessment of this field, we focus on the establishment of material property–catalytic activity relationships. We start with a detailed exploration of prevailing OER mechanisms in acid solution through evaluating the role of catalyst lattice oxygen. We then critically review advances in surface and interface engineering in acidic OER electrocatalysts from both experimental and theoretical perspectives. Finally, a few promising research orientations are proposed to inspire future investigation of high-performance PEM catalysts.

quote

GB/T 7714-2015 [1] Jieqiong Shan, Yao Zheng, Bingyang Shi, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b01758.
MLA [1] Jieqiong Shan, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b01758.
APA [1] Jieqiong Shan, Yao Zheng, Bingyang Shi, Kenneth Davey, & ShiZhang Qiao. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b01758
IEEE [1] Jieqiong Shan, Yao Zheng, Bingyang Shi, Kenneth Davey, and ShiZhang Qiao, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b01758.