Halide Perovskites for Indoor Photovoltaics: The Next Possibility AITranslate
Publisher: ACS
Abstract AITranslate
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.2c02268
Chinese Library Classification Number:
Citation Information:
quote
| GB/T 7714-2015 | [1] Zhanglin Guo, Ajay Kumar Jena, Tsutomu Miyasaka. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02268. |
| MLA | [1] Zhanglin Guo, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02268. |
| APA | [1] Zhanglin Guo, Ajay Kumar Jena, & Tsutomu Miyasaka. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02268 |
| IEEE | [1] Zhanglin Guo, Ajay Kumar Jena, and Tsutomu Miyasaka, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02268. |