Implications of the micromechanical Taylor Factor on work hardening parameters: New perspectives from FFT simulations in DAMASK AITranslate

University of Sheffield; Indian Institute of Technology Roorkee
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Highlights • Classical Taylor model proves inadequate for strain prediction. • Micromechanical Taylor Factor outperforms in capturing local effects. • Work-hardening models improve with Micromechanical Taylor Factor. • Different insights into dislocation mechanisms using refined approach. • Potential to revolutionize materials design with greater precision. This study uses Fast Fourier Transform (FFT) simulations in the Düsseldorf Advanced Material Simulation Kit (DAMASK) to investigate the influence of the micromechanical Taylor Factor on the work hardening parameters. Departing from the assumption of a homogeneous deformation in the classical Taylor model, we use the micromechanical Taylor Factor, which takes better account of local grain interactions and strain distributions. Our comparison of simulations using both classical and micromechanical Taylor factors reveal crucial differences in the predicted dislocation mechanisms, leading to different interpretations of work hardening behavior. Our results question the adequacy of conventional models and suggest a more sophisticated understanding of the deformation of polycrystalline materials. The study underscores the importance of an improved modeling approach to characterize deformation and leads to a re-assessment of existing predictive mechanisms in materials science with possible implications for optimizing of material performance. Graphical abstract Download : Download high-res image (259KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2024.112892

Chinese Library Classification Number:

Citation Information:

Highlights • Classical Taylor model proves inadequate for strain prediction. • Micromechanical Taylor Factor outperforms in capturing local effects. • Work-hardening models improve with Micromechanical Taylor Factor. • Different insights into dislocation mechanisms using refined approach. • Potential to revolutionize materials design with greater precision. This study uses Fast Fourier Transform (FFT) simulations in the Düsseldorf Advanced Material Simulation Kit (DAMASK) to investigate the influence of the micromechanical Taylor Factor on the work hardening parameters. Departing from the assumption of a homogeneous deformation in the classical Taylor model, we use the micromechanical Taylor Factor, which takes better account of local grain interactions and strain distributions. Our comparison of simulations using both classical and micromechanical Taylor factors reveal crucial differences in the predicted dislocation mechanisms, leading to different interpretations of work hardening behavior. Our results question the adequacy of conventional models and suggest a more sophisticated understanding of the deformation of polycrystalline materials. The study underscores the importance of an improved modeling approach to characterize deformation and leads to a re-assessment of existing predictive mechanisms in materials science with possible implications for optimizing of material performance. Graphical abstract Download : Download high-res image (259KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Mirtunjay Kumar, Sumeet Mishra. Computational Materials Science, 2024(237). DOI:10.1016/j.commatsci.2024.112892.
MLA [1] Mirtunjay Kumar, and Sumeet Mishra. Computational Materials Science, no. 237, 2024, https://doi.org/10.1016/j.commatsci.2024.112892.
APA [1] Mirtunjay Kumar, & Sumeet Mishra. (2024). Computational Materials Science(237). https://doi.org/10.1016/j.commatsci.2024.112892
IEEE [1] Mirtunjay Kumar and Sumeet Mishra, Computational Materials Science, no. 237, 2024, doi: 10.1016/j.commatsci.2024.112892.