The cationic ring-opening polymerization of epichlorohydrin co-initiated by BF3•Et2O has been investigated here. Fast synthesis of pure poly(epichlorohydrin) diols (Fn(OH) ≈ 2.0) with controlled molar mass (Mn up to 4000 g mol–1) and low dispersity (Đ < 1.25) was performed both in toluene and in bulk. An original approach was developed here, consisting of first generating in situ the initiator through the BF3•Et2O-catalyzed reaction of ECH with water, leading to a mixture of oligomers with better solubility in the reaction medium than conventional initiators previously used. Then, through a second monomer starved-feed step, polymerization proceeds exclusively through the activated monomer mechanism, allowing perfect control of the polymer growth. The developed procedure was successfully upscaled to 100 g of polymer to validate a future industrial production of PECH, as well as its derivative glycidyl azide polymer (GAP), the most important energetic binder for solid propellants. Additionally, a separate study was performed to elucidate the reasons for coloration of the polymer observed in the course of polymerization and/or under storage.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01105
Chinese Library Classification Number:
Citation Information:
The cationic ring-opening polymerization of epichlorohydrin co-initiated by BF3•Et2O has been investigated here. Fast synthesis of pure poly(epichlorohydrin) diols (Fn(OH) ≈ 2.0) with controlled molar mass (Mn up to 4000 g mol–1) and low dispersity (Đ < 1.25) was performed both in toluene and in bulk. An original approach was developed here, consisting of first generating in situ the initiator through the BF3•Et2O-catalyzed reaction of ECH with water, leading to a mixture of oligomers with better solubility in the reaction medium than conventional initiators previously used. Then, through a second monomer starved-feed step, polymerization proceeds exclusively through the activated monomer mechanism, allowing perfect control of the polymer growth. The developed procedure was successfully upscaled to 100 g of polymer to validate a future industrial production of PECH, as well as its derivative glycidyl azide polymer (GAP), the most important energetic binder for solid propellants. Additionally, a separate study was performed to elucidate the reasons for coloration of the polymer observed in the course of polymerization and/or under storage.
quote
| GB/T 7714-2015 | [1] Georgy V. Timofeev, Maksim I. Hulnik, Irina V. Vasilenko, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01105. |
| MLA | [1] Georgy V. Timofeev, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01105. |
| APA | [1] Georgy V. Timofeev, Maksim I. Hulnik, Irina V. Vasilenko, Francois Ganachaud, Guy Jacob, & Sergei V. Kostjuk. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01105 |
| IEEE | [1] Georgy V. Timofeev, Maksim I. Hulnik, Irina V. Vasilenko, Francois Ganachaud, Guy Jacob, and Sergei V. Kostjuk, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01105. keywords: {cationic ringopening polymerization;living polymerization;poly(epichlorohydrin);functional oligomers;activated monomer;Show More} |