Defect-Rich 2D Material Networks for Advanced Oxygen Evolution Catalysts AITranslate
Abstract AITranslate
A versatile and straightforward room-temperature strategy is demonstrated to synthesize boundary defect-rich ultrathin transition metal hydroxide nanosheet networks by in situ etching of a cobalt metal–organic framework (Co-MOF, ZIF-L-Co). The resultant defect-rich ultrathin Co(OH)2 (D-U-Co(OH)2) nanoarray is one of the most active monometal-based oxygen evolution catalysts to date. Its activity is 3–4 times higher than that of the commercial RuO2 and superior to that of the reported exfoliated bimetallic catalysts. Co-MOF can also be grown on various substrates, and the chemical composition of the defect-rich 2D materials is tunable by changing the metal ions in the etchants. Owing to these merits of the unique synthesis route, our work provides an opportunity for synthesizing advanced nanomaterials that are difficult to get access to by conventional methods.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.8b02343
Chinese Library Classification Number:
Citation Information:
A versatile and straightforward room-temperature strategy is demonstrated to synthesize boundary defect-rich ultrathin transition metal hydroxide nanosheet networks by in situ etching of a cobalt metal–organic framework (Co-MOF, ZIF-L-Co). The resultant defect-rich ultrathin Co(OH)2 (D-U-Co(OH)2) nanoarray is one of the most active monometal-based oxygen evolution catalysts to date. Its activity is 3–4 times higher than that of the commercial RuO2 and superior to that of the reported exfoliated bimetallic catalysts. Co-MOF can also be grown on various substrates, and the chemical composition of the defect-rich 2D materials is tunable by changing the metal ions in the etchants. Owing to these merits of the unique synthesis route, our work provides an opportunity for synthesizing advanced nanomaterials that are difficult to get access to by conventional methods.
quote
| GB/T 7714-2015 | [1] Bowei Zhang, Zhiyuan Qi, Zishan Wu, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.8b02343. |
| MLA | [1] Bowei Zhang, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.8b02343. |
| APA | [1] Bowei Zhang, Zhiyuan Qi, Zishan Wu, Yu Hui Lui, TaeHoon Kim, Xiaohui Tang, Lin Zhou, Wenyu Huang, & Shan Hu. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.8b02343 |
| IEEE | [1] Bowei Zhang, Zhiyuan Qi, Zishan Wu, Yu Hui Lui, TaeHoon Kim, Xiaohui Tang, Lin Zhou, Wenyu Huang, and Shan Hu, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.8b02343. |