daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Alginate–Sodium Sulfate Decahydrate Phase Change Composite with Extended Stability AITranslate

Oak Ridge National Laboratory; Oak Ridge National Laboratory; Oak Ridge National Laboratory; Oak Ridge National Laboratory; Gas Technology Institute; University of Tennessee; Oak Ridge National Laboratory; Oak Ridge National Laboratory; Oak Ridge National Laboratory; Oak Ridge National Laboratory
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This study reports on the use of sodium alginate to effectively stabilize sodium sulfate decahydrate (Na2SO4·10H2O, SSD) based phase change material (PCM) for application as a thermal energy storage material. Alginate/SSD composite PCMs were prepared by blending SSD with different concentrations of alginate polymer. The resulting composite PCMs demonstrate high phase change enthalpy ∼160 J/g and extended cycling stability compared to existing PCM composites. The analysis carried out by optical microscopy, X-ray scattering, and periodic density functional theory (DFT) calculations demonstrated that the stabilization effect was caused by the interplay between ionic and hydrogen bond interactions between the alginate and SSD. Additionally, the variation in mechanical properties of PCM composites with polymer concentrations made it possible to formulate a composite that maintains stable performance after 3D printing. The advanced properties make this composite a promising candidate for application as a thermal energy storage material.

KeyWords AITranslate

polymeric phase change composites sodium sulfate decahydrate sodium alginate thermal energy storage 3D printing
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00933

Chinese Library Classification Number:

Citation Information:

This study reports on the use of sodium alginate to effectively stabilize sodium sulfate decahydrate (Na2SO4·10H2O, SSD) based phase change material (PCM) for application as a thermal energy storage material. Alginate/SSD composite PCMs were prepared by blending SSD with different concentrations of alginate polymer. The resulting composite PCMs demonstrate high phase change enthalpy ∼160 J/g and extended cycling stability compared to existing PCM composites. The analysis carried out by optical microscopy, X-ray scattering, and periodic density functional theory (DFT) calculations demonstrated that the stabilization effect was caused by the interplay between ionic and hydrogen bond interactions between the alginate and SSD. Additionally, the variation in mechanical properties of PCM composites with polymer concentrations made it possible to formulate a composite that maintains stable performance after 3D printing. The advanced properties make this composite a promising candidate for application as a thermal energy storage material.

quote

GB/T 7714-2015 [1] Lingyao Meng, Alexander S. Ivanov, Sungjin Kim, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00933.
MLA [1] Lingyao Meng, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00933.
APA [1] Lingyao Meng, Alexander S. Ivanov, Sungjin Kim, Xiao Zhao, Navin Kumar, Amanda YoungGonzales, Tomonori Saito, Wim Bras, Kyle Gluesenkamp, & Vera Bocharova. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00933
IEEE [1] Lingyao Meng, Alexander S. Ivanov, Sungjin Kim, Xiao Zhao, Navin Kumar, Amanda YoungGonzales, Tomonori Saito, Wim Bras, Kyle Gluesenkamp, and Vera Bocharova, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00933. keywords: {polymeric phase change composites;sodium sulfate decahydrate;sodium alginate;thermal energy storage;3D printing}