Structural, elastic, electronic, chemical bonding and optical properties of Cu-based oxides ACuO (A = Li, Na, K and Rb): An ab initio study AITranslate
Abstract AITranslate
Highlights • Elastic and optical properties of ACuO materials have been predicted. • Additional data about electronic properties have provided. • Pressure dependences of structural, bonds and elastic constants have been analyzed. • These materials show structural and elastic anisotropy, and an optical isotropy. Ab initio total energy calculations were performed to study in details the structural, elastic, electronic, chemical bonding and optical properties of Cu-based ternary oxides ACuO (A = Li, Na, K and Rb). Optimized atomic coordinates and lattice constants agree well with the existing experimental and theoretical data. Numerical estimations of the six independent elastic constants Cij and their related properties for monocrystalline ACuO were obtained. A set of elastic moduli for polycrystalline ACuO, namely bulk modulus B, shear modulus G, Young’s modulus E, Poisson’s ratio σ, Lamé coefficients λ and Debye temperature θD were evaluated. Band structure, total and site-projected l-decomposed densities of states, charge-carrier effective masses, charge transfers and charge density distribution maps were obtained; analyzed and compared with the available theoretical data. Complex dielectric function, refractive index, extinction coefficient, reflectivity and loss function spectra were calculated with an incident radiation polarized parallel to both [1 0 0] and [0 0 1] crystalline directions.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2013.09.011
Chinese Library Classification Number:
Citation Information:
Highlights • Elastic and optical properties of ACuO materials have been predicted. • Additional data about electronic properties have provided. • Pressure dependences of structural, bonds and elastic constants have been analyzed. • These materials show structural and elastic anisotropy, and an optical isotropy. Ab initio total energy calculations were performed to study in details the structural, elastic, electronic, chemical bonding and optical properties of Cu-based ternary oxides ACuO (A = Li, Na, K and Rb). Optimized atomic coordinates and lattice constants agree well with the existing experimental and theoretical data. Numerical estimations of the six independent elastic constants Cij and their related properties for monocrystalline ACuO were obtained. A set of elastic moduli for polycrystalline ACuO, namely bulk modulus B, shear modulus G, Young’s modulus E, Poisson’s ratio σ, Lamé coefficients λ and Debye temperature θD were evaluated. Band structure, total and site-projected l-decomposed densities of states, charge-carrier effective masses, charge transfers and charge density distribution maps were obtained; analyzed and compared with the available theoretical data. Complex dielectric function, refractive index, extinction coefficient, reflectivity and loss function spectra were calculated with an incident radiation polarized parallel to both [1 0 0] and [0 0 1] crystalline directions.
quote
| GB/T 7714-2015 | [1] A. Bouhemadou, O. Boudrifa, N. Guechi, et al. Computational Materials Science, 2014(81). DOI:10.1016/j.commatsci.2013.09.011. |
| MLA | [1] A. Bouhemadou, et al., Computational Materials Science, no. 81, 2014, https://doi.org/10.1016/j.commatsci.2013.09.011. |
| APA | [1] A. Bouhemadou, O. Boudrifa, N. Guechi, R. Khenata, Y. AlDouri, Ş. Uğur, B. Ghebouli, & S. BinOmran. (2014). Computational Materials Science(81). https://doi.org/10.1016/j.commatsci.2013.09.011 |
| IEEE | [1] A. Bouhemadou, O. Boudrifa, N. Guechi, R. Khenata, Y. AlDouri, Ş. Uğur, B. Ghebouli, and S. BinOmran, Computational Materials Science, no. 81, 2014, doi: 10.1016/j.commatsci.2013.09.011. |