Abstract AITranslate

In this study, we present the fabrication of a two-step thermoresponsive ultrafiltration (UF) membrane through polymerization of a lyotropic liquid crystal (LLC). A mixture of commercially available Pluronic F127 block copolymer, water (containing ammonium persulfate as the initiator), and polymerizable oil (n-butyl acrylate/ethylene glycol dimethacrylate) is used to create an LLC with a lamellar structure, as characterized by cross-polarized light microscopy and atomic force microscopy. Differential scanning calorimetry is employed to evaluate the thermoresponsive behavior of the polymerized LLC (polyLLC). Two-step thermoresponsiveness (∼35 and ∼50 °C) of the polyLLC is observed due to the lower critical solution temperature (LCST) of F127 and melting of the crystalline structure of the polyethylene oxide (PEO) chains of the F127 surfactant. In the next step, the obtained mesophase is cast on a nonwoven polyester support sheet followed by thermal polymerization. The hydration capacity, water flux, water flux recovery after fouling, and molecular weight cutoff (MWCO) of the obtained membrane are evaluated at different temperatures to examine its thermoresponsiveness. The experimental results reveal that the UF membrane has a reversible thermoresponsive behavior at the LCST and PEO melting of polyLLC. Additionally, the cleaning efficiency of the fouled membrane can be enhanced by using its thermoresponsive behavior, resulting in an extended lifetime of the product. Furthermore, the MWCO of the membrane can be altered with temperature due to the pore size change with temperature stimulus.

KeyWords AITranslate

thermoresponsive membranes lyotropic liquid crystals mesophases thermal polymerization selfassembly
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01095

Chinese Library Classification Number:

Citation Information:

In this study, we present the fabrication of a two-step thermoresponsive ultrafiltration (UF) membrane through polymerization of a lyotropic liquid crystal (LLC). A mixture of commercially available Pluronic F127 block copolymer, water (containing ammonium persulfate as the initiator), and polymerizable oil (n-butyl acrylate/ethylene glycol dimethacrylate) is used to create an LLC with a lamellar structure, as characterized by cross-polarized light microscopy and atomic force microscopy. Differential scanning calorimetry is employed to evaluate the thermoresponsive behavior of the polymerized LLC (polyLLC). Two-step thermoresponsiveness (∼35 and ∼50 °C) of the polyLLC is observed due to the lower critical solution temperature (LCST) of F127 and melting of the crystalline structure of the polyethylene oxide (PEO) chains of the F127 surfactant. In the next step, the obtained mesophase is cast on a nonwoven polyester support sheet followed by thermal polymerization. The hydration capacity, water flux, water flux recovery after fouling, and molecular weight cutoff (MWCO) of the obtained membrane are evaluated at different temperatures to examine its thermoresponsiveness. The experimental results reveal that the UF membrane has a reversible thermoresponsive behavior at the LCST and PEO melting of polyLLC. Additionally, the cleaning efficiency of the fouled membrane can be enhanced by using its thermoresponsive behavior, resulting in an extended lifetime of the product. Furthermore, the MWCO of the membrane can be altered with temperature due to the pore size change with temperature stimulus.

quote

GB/T 7714-2015 [1] Younes Saadat, Kyungtae Kim, Reza Foudazi. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01095.
MLA [1] Younes Saadat, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01095.
APA [1] Younes Saadat, Kyungtae Kim, & Reza Foudazi. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01095
IEEE [1] Younes Saadat, Kyungtae Kim, and Reza Foudazi, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01095. keywords: {thermoresponsive membranes;lyotropic liquid crystals;mesophases;thermal polymerization;selfassembly}