daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Single-Ion Conducting Multi-block Copolymer Electrolyte for Lithium-Metal Batteries with High Mass Loading NCM811 Cathodes AITranslate

Germany|Karlsruhe Institute of Technology (KIT); Germany|Karlsruhe Institute of Technology (KIT); Germany|Karlsruhe Institute of Technology (KIT); Germany|Karlsruhe Institute of Technology (KIT); Germany|Karlsruhe Institute of Technology (KIT)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lithium-metal batteries comprising a single-ion conducting polymer electrolyte and a nickel-rich LiNi1-x-yCoxMnyO2 (NCM) positive electrode (cathode) potentially offer very high energy density and great safety. However, such cell chemistry is very demanding concerning the required interfacial stability of the polymer electrolyte, and the realization of high mass loading cathodes remains a great challenge. Herein, the development of a new single-ion conducting multi-block copolymer electrolyte including trifluoromethyl groups in the ionophilic block is reported. After ethylene carbonate (EC) is incorporated into the self-standing and easily processable polymer membranes, high ionic conductivity along with very high limiting current density and suitable anodic stability are obtained. These enable stable cycling of Li∥NCM811 cells─also at high C rates (up to 5C) and active material mass loadings of the NCM811 cathode of >10 mg cm–2, which are both key steps toward the potential commercialization of this class of electrolytes.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.2c02806

Chinese Library Classification Number:

Citation Information:

Lithium-metal batteries comprising a single-ion conducting polymer electrolyte and a nickel-rich LiNi1-x-yCoxMnyO2 (NCM) positive electrode (cathode) potentially offer very high energy density and great safety. However, such cell chemistry is very demanding concerning the required interfacial stability of the polymer electrolyte, and the realization of high mass loading cathodes remains a great challenge. Herein, the development of a new single-ion conducting multi-block copolymer electrolyte including trifluoromethyl groups in the ionophilic block is reported. After ethylene carbonate (EC) is incorporated into the self-standing and easily processable polymer membranes, high ionic conductivity along with very high limiting current density and suitable anodic stability are obtained. These enable stable cycling of Li∥NCM811 cells─also at high C rates (up to 5C) and active material mass loadings of the NCM811 cathode of >10 mg cm–2, which are both key steps toward the potential commercialization of this class of electrolytes.

quote

GB/T 7714-2015 [1] Xu Dong, Alexander Mayer, Xu Liu, et al. ACS Energy Letters, 2023(8). DOI:10.1021/acsenergylett.2c02806.
MLA [1] Xu Dong, et al., ACS Energy Letters, no. 8, 2023, https://doi.org/10.1021/acsenergylett.2c02806.
APA [1] Xu Dong, Alexander Mayer, Xu Liu, Stefano Passerini, & Dominic Bresser. (2023). ACS Energy Letters(8). https://doi.org/10.1021/acsenergylett.2c02806
IEEE [1] Xu Dong, Alexander Mayer, Xu Liu, Stefano Passerini, and Dominic Bresser, ACS Energy Letters, no. 8, 2023, doi: 10.1021/acsenergylett.2c02806.