Abstract AITranslate

This review article sheds useful insight in the use of Janus nanoparticles for (bio)sensing in connection with optical and electrochemical transduction. After a brief introduction of the main properties, types and fabrication strategies of Janus nanoparticles, selected applications for their use in electrochemical and optical biosensing are critically discussed. Highlighted examples illustrate the great versatility and interesting possibilities offered by these smart multifunctional nanoparticles for (bio)sensing of relevant analytes operating both in static and dynamic modes. Progress made so far demonstrate their suitability for designing single- or multiplexed (bio)sensing strategies for target analytes of different nature (organic and inorganic compounds, proteins, cells and oligomers) with relevance in clinical (H2O2, glucose, cholesterol, CEA, human IgG, propranolol, bacterial and tumor cells) and environmental (lead and organophosphorous nerve agents) fields. Key future challenges and envisioned opportunities of the use of Janus nanoparticles in the (bio)sensing field are also discussed. Graphical abstract Download : Download high-res image (158KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.apmt.2017.08.004

Chinese Library Classification Number:

Citation Information:

This review article sheds useful insight in the use of Janus nanoparticles for (bio)sensing in connection with optical and electrochemical transduction. After a brief introduction of the main properties, types and fabrication strategies of Janus nanoparticles, selected applications for their use in electrochemical and optical biosensing are critically discussed. Highlighted examples illustrate the great versatility and interesting possibilities offered by these smart multifunctional nanoparticles for (bio)sensing of relevant analytes operating both in static and dynamic modes. Progress made so far demonstrate their suitability for designing single- or multiplexed (bio)sensing strategies for target analytes of different nature (organic and inorganic compounds, proteins, cells and oligomers) with relevance in clinical (H2O2, glucose, cholesterol, CEA, human IgG, propranolol, bacterial and tumor cells) and environmental (lead and organophosphorous nerve agents) fields. Key future challenges and envisioned opportunities of the use of Janus nanoparticles in the (bio)sensing field are also discussed. Graphical abstract Download : Download high-res image (158KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] P. YánezSedeño, S. Campuzano, J.M. Pingarrón. Applied Materials Today, 2017(9). DOI:10.1016/j.apmt.2017.08.004.
MLA [1] P. YánezSedeño, et al., Applied Materials Today, no. 9, 2017, https://doi.org/10.1016/j.apmt.2017.08.004.
APA [1] P. YánezSedeño, S. Campuzano, & J.M. Pingarrón. (2017). Applied Materials Today(9). https://doi.org/10.1016/j.apmt.2017.08.004
IEEE [1] P. YánezSedeño, S. Campuzano, and J.M. Pingarrón, Applied Materials Today, no. 9, 2017, doi: 10.1016/j.apmt.2017.08.004.