daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Thick TiO2-Based Top Electron Transport Layer on Perovskite for Highly Efficient and Stable Solar Cells AITranslate

The University of Hong Kong; The University of Hong Kong; The University of Hong Kong; The University of Hong Kong; The University of Hong Kong; The University of Hong Kong; The University of Hong Kong; The Hong Kong Baptist University; City University of Hong Kong; The University of Hong Kong
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Simultaneously achieving high efficiency, long-term stability, and robust fabrication with good reproducibility in perovskite solar cells (PVSCs) is essential for their practical applications. Herein, we first demonstrate a thick TiO2 backbone film directly on top of a perovskite film through a simple room-temperature solution process. Through the strategy of decorating the TiO2 film with fullerene for passivating traps and filling voids, we achieve a fullerene-decorated TiO2 electron transport layer (ETL) in inverted PVSCs. Because of the suppressed monomolecular Shockley–Read–Hall recombination and ion diffusion of the fullerene-decorated TiO2 ETL, stabilized efficiencies of ∼20% and shelf life stability remaining over 98% of initial efficiency after aging in ambient conditions or 16 months are achieved. Remarkably, the PVSCs are insensitive to TiO2 thickness from 50 to 250 nm, which contributes significantly to the robust fabrication and high reproducibility of the PVSCs. This work provides an ETL design on top of a perovskite film for simultaneous improvement of PVSC efficiency, stability, and reproducibility.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsenergylett.8b01507

Chinese Library Classification Number:

Citation Information:

Simultaneously achieving high efficiency, long-term stability, and robust fabrication with good reproducibility in perovskite solar cells (PVSCs) is essential for their practical applications. Herein, we first demonstrate a thick TiO2 backbone film directly on top of a perovskite film through a simple room-temperature solution process. Through the strategy of decorating the TiO2 film with fullerene for passivating traps and filling voids, we achieve a fullerene-decorated TiO2 electron transport layer (ETL) in inverted PVSCs. Because of the suppressed monomolecular Shockley–Read–Hall recombination and ion diffusion of the fullerene-decorated TiO2 ETL, stabilized efficiencies of ∼20% and shelf life stability remaining over 98% of initial efficiency after aging in ambient conditions or 16 months are achieved. Remarkably, the PVSCs are insensitive to TiO2 thickness from 50 to 250 nm, which contributes significantly to the robust fabrication and high reproducibility of the PVSCs. This work provides an ETL design on top of a perovskite film for simultaneous improvement of PVSC efficiency, stability, and reproducibility.

quote

GB/T 7714-2015 [1] Yong Zhao, Hong Zhang, Xingang Ren, et al. ACS Energy Letters, 2018(3). DOI:10.1021/acsenergylett.8b01507.
MLA [1] Yong Zhao, et al., ACS Energy Letters, no. 3, 2018, https://doi.org/10.1021/acsenergylett.8b01507.
APA [1] Yong Zhao, Hong Zhang, Xingang Ren, Hugh L. Zhu, Zhanfeng Huang, Fei Ye, Dan Ouyang, Kok Wai Cheah, Alex K.Y. Jen, & Wallace C. H. Choy. (2018). ACS Energy Letters(3). https://doi.org/10.1021/acsenergylett.8b01507
IEEE [1] Yong Zhao, Hong Zhang, Xingang Ren, Hugh L. Zhu, Zhanfeng Huang, Fei Ye, Dan Ouyang, Kok Wai Cheah, Alex K.Y. Jen, and Wallace C. H. Choy, ACS Energy Letters, no. 3, 2018, doi: 10.1021/acsenergylett.8b01507.