Acid-Resistant Polyimide Ultrafiltration Membranes for Direct Separation of Lignin from Deep Eutectic Solvents AITranslate

University of Chinese Academy of Sciences; Changzhou University; Nanjing Tech University; University of Chinese Academy of Sciences; Institute of Process Engineering; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences; University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Direct separation of lignin from fully acidic deep eutectic solvent (DES) is challenging because of its high viscosity and acidity. In this study, three synthesized DES-resistant polyimides (PIs), namely, B-PI, 6F-PI, and P-PI based on 4′,6-diamidino-2-phenylindole (DAPI) with 4,4′-(4,4′-isopropylidenediphenoxy)bis-(phthalic anhydride) (BPADA), 4,4′-(hexafluoroisopropylidene)diphthalic anhydride (6FDA) and pyromellitic dianhydride (PMDA), respectively, were used to prepare ultrafiltration (UF) membranes for the direct separation of sodium lignosulfonate (LS) from its DES (choline chloride:lactic acid) solutions for the first time. The morphology, pore size, surface property, degree of swelling, LS separation performance, and long-term stability of the resulting UF membranes were investigated in detail. The average pore sizes were in the range of 3.60–5.06 nm, and the LS rejections, as well as the DES fluxes, were 44.0–66.4% and 4.71–16.55 L·m–2 h–1, respectively, both higher than those from commercial ZrO2/TiO2 membrane (25.6% and 1.91 L·m–2 h–1). Among them, the B-PI membrane had the best separation performance and excellent operating stability for 20 h due to its low fractional free volume and poor affinity with DES. Swelling and positive charges of membrane surface in the DES system decreased LS rejection. In addition, a higher degree of swelling and affinity with DES led to an increased DES flux when compared with the aqueous system. Herein the PI-based UF membranes are promising for the direct lignin separation process, especially in an acidic DES system.

KeyWords AITranslate

polyimides ultrafiltration membranes lignin deep eutectic solvents
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00940

Chinese Library Classification Number:

Citation Information:

Direct separation of lignin from fully acidic deep eutectic solvent (DES) is challenging because of its high viscosity and acidity. In this study, three synthesized DES-resistant polyimides (PIs), namely, B-PI, 6F-PI, and P-PI based on 4′,6-diamidino-2-phenylindole (DAPI) with 4,4′-(4,4′-isopropylidenediphenoxy)bis-(phthalic anhydride) (BPADA), 4,4′-(hexafluoroisopropylidene)diphthalic anhydride (6FDA) and pyromellitic dianhydride (PMDA), respectively, were used to prepare ultrafiltration (UF) membranes for the direct separation of sodium lignosulfonate (LS) from its DES (choline chloride:lactic acid) solutions for the first time. The morphology, pore size, surface property, degree of swelling, LS separation performance, and long-term stability of the resulting UF membranes were investigated in detail. The average pore sizes were in the range of 3.60–5.06 nm, and the LS rejections, as well as the DES fluxes, were 44.0–66.4% and 4.71–16.55 L·m–2 h–1, respectively, both higher than those from commercial ZrO2/TiO2 membrane (25.6% and 1.91 L·m–2 h–1). Among them, the B-PI membrane had the best separation performance and excellent operating stability for 20 h due to its low fractional free volume and poor affinity with DES. Swelling and positive charges of membrane surface in the DES system decreased LS rejection. In addition, a higher degree of swelling and affinity with DES led to an increased DES flux when compared with the aqueous system. Herein the PI-based UF membranes are promising for the direct lignin separation process, especially in an acidic DES system.

quote

GB/T 7714-2015 [1] Jing Li, Jian Lu, Haoqi Sang, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00940.
MLA [1] Jing Li, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00940.
APA [1] Jing Li, Jian Lu, Haoqi Sang, Yu Zhang, Benkun Qi, Jianquan Luo, Yinhua Wan, & Yongbing Zhuang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00940
IEEE [1] Jing Li, Jian Lu, Haoqi Sang, Yu Zhang, Benkun Qi, Jianquan Luo, Yinhua Wan, and Yongbing Zhuang, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00940. keywords: {polyimides;ultrafiltration;membranes;lignin;deep eutectic solvents}