Interlayer Interaction Enhancement in Ruddlesden–Popper Perovskite Solar Cells toward High Efficiency and Phase Stability AITranslate
Abstract AITranslate
Ruddlesden–Popper perovskites (RPPs) have attracted intense attention owing to their superior stability. However, the interspace and weak interaction between the inorganic layers inhibits direct charge transfer and brings the phase segregation issue under light illumination. Herein, it is presented that after incorporation of a symmetric cation guanidinium (GA+) with three amino groups the crystallinity, photoelectronic properties, and stability can be synchronously ameliorated owning to the enhanced interlayer interaction. The new (BA,GA)2(MA)2Pb3I10 RPP film shows a preferentially vertical orientation and possesses a spatially well-aligned band from the bottom to the top surface, resulting in fast energy transfer. It contributes to a large Voc of 1.25 V with minimized nonradiative loss of 0.14 V and a boosted efficiency of 14.47%. More importantly, the lattice strain in the RPP film can be eliminated due to the medium size of GA+, protecting it from phase segregation even under laser irradiation.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsenergylett.9b00351
Chinese Library Classification Number:
Citation Information:
Ruddlesden–Popper perovskites (RPPs) have attracted intense attention owing to their superior stability. However, the interspace and weak interaction between the inorganic layers inhibits direct charge transfer and brings the phase segregation issue under light illumination. Herein, it is presented that after incorporation of a symmetric cation guanidinium (GA+) with three amino groups the crystallinity, photoelectronic properties, and stability can be synchronously ameliorated owning to the enhanced interlayer interaction. The new (BA,GA)2(MA)2Pb3I10 RPP film shows a preferentially vertical orientation and possesses a spatially well-aligned band from the bottom to the top surface, resulting in fast energy transfer. It contributes to a large Voc of 1.25 V with minimized nonradiative loss of 0.14 V and a boosted efficiency of 14.47%. More importantly, the lattice strain in the RPP film can be eliminated due to the medium size of GA+, protecting it from phase segregation even under laser irradiation.
quote
| GB/T 7714-2015 | [1] Mingzhu Long, Tiankai Zhang, Dongcheng Chen, et al. ACS Energy Letters, 2019(4). DOI:10.1021/acsenergylett.9b00351. |
| MLA | [1] Mingzhu Long, et al., ACS Energy Letters, no. 4, 2019, https://doi.org/10.1021/acsenergylett.9b00351. |
| APA | [1] Mingzhu Long, Tiankai Zhang, Dongcheng Chen, Minchao Qin, Zefeng Chen, Li Gong, Xinhui Lu, Fangyan Xie, Weiguang Xie, Jian Chen, & Jianbin Xu. (2019). ACS Energy Letters(4). https://doi.org/10.1021/acsenergylett.9b00351 |
| IEEE | [1] Mingzhu Long, Tiankai Zhang, Dongcheng Chen, Minchao Qin, Zefeng Chen, Li Gong, Xinhui Lu, Fangyan Xie, Weiguang Xie, Jian Chen, and Jianbin Xu, ACS Energy Letters, no. 4, 2019, doi: 10.1021/acsenergylett.9b00351. |