Ravenna Grass-Extracted Alkaline Lignin-Based Polysulfone Mixed Matrix Membrane (MMM) for Aqueous Cr(VI) Removal AITranslate

Indian Institute of Technology Guwahati; Indian Institute of Technology Guwahati; Indian Institute of Technology Guwahati; Indian Institute of Technology Guwahati; Indian Institute of Technology Guwahati
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Studies have suggested that ecofriendly, inexpensive, and renewable material sources are essential for developing scalable, high-performance mixed matrix membranes (MMMs). With the fact that the second-most prevalent biomacromolecule in the world of plant biology is lignin, this article delineates the effective fabrication of a lignin-based MMM utilizing polysulfone (PSf) as the base material. The influence of PSf and the lignin concentration on the properties of the fabricated membranes was examined. Also, the developed membranes were assessed for surface morphology, roughness, thickness, thermal stability, functional groups, elemental composition, mechanical strength, and hydrophilicity. Atomic force microscopy (AFM) and scanning electron microscopy (SEM) studies showed that the PSf/lignin membranes possessed a rough and inconsistent morphology and comparatively greater surface porosity. The water contact angle was reduced for the 1.0 wt % PSF/lignin membrane. Furthermore, lignin nanoparticles significantly impacted the membrane surface characteristics and decreased the ζ potential. Under the ideal experimental scenario, M2 (0.5 wt % lignin/PSf) and M3 (1.0 wt % lignin/PSf) membranes demonstrated good pure water flux values and a higher removal of 98.5 and 98.75% of Cr(VI), respectively. EDX analysis of the membranes after filtration affirmed the effective Cr(VI) removal from water. Owing to its low cost, green credentials, simplicity in synthesis, and remarkable efficiency, the newly developed PSf/lignin membrane is best suited for removing Cr(VI) and various other related contaminants from discharge aqueous effluents.

KeyWords AITranslate

alkaline lignin mixed matrix membrane polysulfone membrane Cr(VI) removal water treatment
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c00999

Chinese Library Classification Number:

Citation Information:

Studies have suggested that ecofriendly, inexpensive, and renewable material sources are essential for developing scalable, high-performance mixed matrix membranes (MMMs). With the fact that the second-most prevalent biomacromolecule in the world of plant biology is lignin, this article delineates the effective fabrication of a lignin-based MMM utilizing polysulfone (PSf) as the base material. The influence of PSf and the lignin concentration on the properties of the fabricated membranes was examined. Also, the developed membranes were assessed for surface morphology, roughness, thickness, thermal stability, functional groups, elemental composition, mechanical strength, and hydrophilicity. Atomic force microscopy (AFM) and scanning electron microscopy (SEM) studies showed that the PSf/lignin membranes possessed a rough and inconsistent morphology and comparatively greater surface porosity. The water contact angle was reduced for the 1.0 wt % PSF/lignin membrane. Furthermore, lignin nanoparticles significantly impacted the membrane surface characteristics and decreased the ζ potential. Under the ideal experimental scenario, M2 (0.5 wt % lignin/PSf) and M3 (1.0 wt % lignin/PSf) membranes demonstrated good pure water flux values and a higher removal of 98.5 and 98.75% of Cr(VI), respectively. EDX analysis of the membranes after filtration affirmed the effective Cr(VI) removal from water. Owing to its low cost, green credentials, simplicity in synthesis, and remarkable efficiency, the newly developed PSf/lignin membrane is best suited for removing Cr(VI) and various other related contaminants from discharge aqueous effluents.

quote

GB/T 7714-2015 [1] Simons Dhara, Niladri Shekhar Samanta, Pranjal P. Das, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c00999.
MLA [1] Simons Dhara, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c00999.
APA [1] Simons Dhara, Niladri Shekhar Samanta, Pranjal P. Das, Ramagopal Venkata Sai Uppaluri, & Mihir K. Purkait. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c00999
IEEE [1] Simons Dhara, Niladri Shekhar Samanta, Pranjal P. Das, Ramagopal Venkata Sai Uppaluri, and Mihir K. Purkait, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c00999. keywords: {alkaline lignin;mixed matrix membrane;polysulfone membrane;Cr(VI) removal;water treatment}