Injectable Poly(oligoethylene glycol methacrylate)-Based Hydrogels Fabricated from Highly Branched Precursor Polymers: Controlling Gel Properties by Precursor Polymer Morphology AITranslate
Abstract AITranslate
The physicochemical properties of injectable hydrogels are typically modified by altering the chemistry of the precursor polymer and/or the amount or type of cross-linker, both of which can lead to hydrogels with altered mechanics, swelling, degradation, and other key physical properties. Herein, we describe an alternative approach to tune the properties of injectable hydrogels (here, based on hydrazone cross-linked poly(oligoethylene glycol methacrylate), or POEGMA) by altering the architecture of the precursor polymers through branching. Hydrogels prepared using highly branched precursor polymers had nearly identical chemical compositions but exhibited markedly different physical properties relative to linear precursor hydrogels on which we have previously reported. Specifically, increasing the degree of branching resulted in increased degradation time and stiffness but decreased gelation time and gel swelling. The mechanical properties of highly branched hydrogels are relatively insensitive to the mass concentration of precursor polymer used to prepare the gels, in contrast to hydrogels prepared with linear precursors; furthermore, gels prepared from only highly branched precursors exhibit substantially prolonged degradation times compared to all-linear or linear–highly branched hydrogels. Overall, introducing branching in the precursor polymers is demonstrated to provide an alternate strategy to tune injectable hydrogel properties while decoupling otherwise coupled properties (e.g., polymer concentration and mechanics).
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.8b00085
Chinese Library Classification Number:
Citation Information:
The physicochemical properties of injectable hydrogels are typically modified by altering the chemistry of the precursor polymer and/or the amount or type of cross-linker, both of which can lead to hydrogels with altered mechanics, swelling, degradation, and other key physical properties. Herein, we describe an alternative approach to tune the properties of injectable hydrogels (here, based on hydrazone cross-linked poly(oligoethylene glycol methacrylate), or POEGMA) by altering the architecture of the precursor polymers through branching. Hydrogels prepared using highly branched precursor polymers had nearly identical chemical compositions but exhibited markedly different physical properties relative to linear precursor hydrogels on which we have previously reported. Specifically, increasing the degree of branching resulted in increased degradation time and stiffness but decreased gelation time and gel swelling. The mechanical properties of highly branched hydrogels are relatively insensitive to the mass concentration of precursor polymer used to prepare the gels, in contrast to hydrogels prepared with linear precursors; furthermore, gels prepared from only highly branched precursors exhibit substantially prolonged degradation times compared to all-linear or linear–highly branched hydrogels. Overall, introducing branching in the precursor polymers is demonstrated to provide an alternate strategy to tune injectable hydrogel properties while decoupling otherwise coupled properties (e.g., polymer concentration and mechanics).
quote
| GB/T 7714-2015 | [1] Ivan Urosev, Helen Dorrington, Nicola Muzzin, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.8b00085. |
| MLA | [1] Ivan Urosev, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.8b00085. |
| APA | [1] Ivan Urosev, Helen Dorrington, Nicola Muzzin, Richard Alsop, Emilia Bakaic, Trevor Gilbert, Maikel Rheinstädter, & Todd Hoare. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.8b00085 |
| IEEE | [1] Ivan Urosev, Helen Dorrington, Nicola Muzzin, Richard Alsop, Emilia Bakaic, Trevor Gilbert, Maikel Rheinstädter, and Todd Hoare, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.8b00085. keywords: {highly branched polymers;hydrogel;in situ gelling;poly(oligoethylene glycol methacrylate);injectable} |